Er:YAG laser, piezosurgery, and surgical drill for bone decortication during orthodontic mini-implant insertion: primary stability analysis-an animal study.
Matys, Jacek; Flieger, Rafal; Tenore, Gianluca; Grzech-Lesniak, Kinga; Romeo, Umberto; Dominiak, Marzena.
Afiliação
  • Matys J; "Sapienza" University of Rome, Rome, Italy. jacek.matys@wp.pl.
  • Flieger R; Private Dental Healthcare, Lipowa 18, 67-400, Wschowa, Poland. jacek.matys@wp.pl.
  • Tenore G; Private Dental Healthcare, Koscian, Poland.
  • Grzech-Lesniak K; Department of Oral and Maxillofacial Sciences, "Sapienza" University of Rome, Rome, Italy.
  • Romeo U; Dental Surgery Department, Medical University of Wroclaw, Wroclaw, Poland.
  • Dominiak M; Department of Oral and Maxillofacial Sciences, "Sapienza" University of Rome, Rome, Italy.
Lasers Med Sci ; 33(3): 489-495, 2018 Apr.
Article em En | MEDLINE | ID: mdl-29127605
ABSTRACT
It is important to identify factors that affect primary stability of orthodontic mini-implants because it determines the success of treatment. We assessed mini-implant primary stability (initial mechanical engagement with the bone) placed in pig jaws. We also assessed mini-implant insertion failure rate (mini-implant fracture, mini-implants to root contact). A total of 80 taper-shaped mini-implants (Absoanchor® Model SH1312-6; Dentos Inc., Daegu, Korea) 6 mm long with a diameter of 1.1 mm were used. Bone decortication was made before mini-implant insertion by means of three different

methods:

Group G1 ErYAG laser (LiteTouch®, Light Instruments, Yokneam, Israel) at energy of 300 mJ, frequency 25 Hz, fluence 38.2 J/cm2, cooling 14 ml/min, tip 1.0 × 17 mm, distance 1 mm, time of irradiation 6 s; Group G2 drill (Hager & Meisinger GmbH, Hansemannstr, Germany); Group G3 piezosurgery (Piezotom Solo, Acteon, NJ, USA). In G4 group (control), mini-implants were driven by a self-drilling method. The primary stability of mini-implants was assessed by measuring damping characteristics between the implant and the tapping head of Periotest device (Gulden-Medizinteknik, Eschenweg, Modautal, Germany). The results in range between - 8 to + 9 allowed immediate loading. Significantly lower Periotest value was found in the control group (mean 0.59 ± 1.57, 95% CI 0.7, 2.4) as compared with ErYAG laser (mean 4.44 ± 1.64, 95% CI 3.6, 5.3), piezosurgery (mean 17.92 ± 2.73, 95% CI 16.5, 19.3), and a drill (mean 5.91 ± 1.52, 95% CI 5.2, 6.6) (p < 0.05). The highest failure rate (33.3%) during mini-implant insertion was noted for self-drilling method (G4) as compared with G1, G2, and G3 groups (p < 0.05). The small diameter decortication by ErYAG laser appeared to provide better primary stability as compared to drill and piezosurgery. Decortication of the cortical bone before mini-implant insertion resulted in reduced risk of implant fracture or injury of adjacent teeth. The high initial stability with a smaller diameter of the mini-implant resulted in increased risk of fracture, especially for a self-drilling method.
Assuntos
Palavras-chave

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Ortodontia / Osso e Ossos / Implantes Dentários / Lasers de Estado Sólido / Piezocirurgia Tipo de estudo: Prognostic_studies Limite: Animals Idioma: En Ano de publicação: 2018 Tipo de documento: Article

Texto completo: 1 Base de dados: MEDLINE Assunto principal: Ortodontia / Osso e Ossos / Implantes Dentários / Lasers de Estado Sólido / Piezocirurgia Tipo de estudo: Prognostic_studies Limite: Animals Idioma: En Ano de publicação: 2018 Tipo de documento: Article