<p><b>OBJECTIVE</b>To study the effect of repeated firings on color of porcelain-fused-to-titanium restorations.</p><p><b>METHODS</b>Twenty standard porcelain-fused-to-titanium specimens were made with Dentsply DETREY TiBond C3 and Dentaurum rematitan Til. Then they were fired 1, 2, 4, 7, and 10 times. Color measurement was done after each firing.</p><p><b>RESULT</b>Most of the color parameters had no significant difference after firing except for a* and Hab. All the color difference among groups were smaller than 1.0 (deltaE < 1.0).</p><p><b>CONCLUSION</b>Repeated firings will not affect the color stability of porcelain-fused-to-titanium restorations.</p>
Full text:
Available
Index:
WPRIM (Western Pacific)
Main subject:
Reference Standards
/
Titanium
/
Denture Design
/
Metal Ceramic Alloys
/
Prosthesis Coloring
/
Color
/
Dental Porcelain
/
Methods
Limits:
Humans
Language:
Chinese
Journal:
Acta Academiae Medicinae Sinicae
Year:
2004
Type:
Article
Similar
MEDLINE
...
LILACS
LIS