Comparison of mechanical properties in 4 indirect composite resin / 대한치과보철학회지
Article de Ko | WPRIM | ID: wpr-20209
Bibliothèque responsable: WPRO
ABSTRACT
STATEMENT OF PROBLEM: The esthetic component of dental care has become increasingly more important, while new tooth-colored materials are continually marketed. Various new indirect composite materials have been developed with required advantages. The most recent development in the indirect composites has been the introduction of the second-generation laboratory composite or poly-glass materials. They are processed by different laboratory techniques based on combinations of heat, pressure, vacuum and light polymerization. Although, second generation products became available in 1995, their characteristics and clinical performance have not been adequately investigated. PURPOSE: The aim of this study was to measure the mechanical properties of the second generation indirect resin system and compare these with an existing universal direct composite resin. MATERIAL AND METHOD: In this study four indirect composite material (Adoro LC, BelleGlass HP, Tescera, Synfony) were tested for flexural strength, wear resistance, hardness and their degree of conversion against Z250, a light cure direct composite. RESULTS: Within the limitations of this study, the following conclusions were drawn: 1. From the abrasion wear result, Adoro showed the least volume loss while Synfony showed the greatest volume loss. Z250 and BelleGlass HP didn't show significant difference (p>0.05), but they showed significant difference with other groups (p0.05). While Synfony showed the greatest volume loss that it showed significant difference with other groups (p>0.05). 2. Mean values of flexural strength by means of three point bending test was in the order of Z250, Adoro, Belleglass HP, Tescera and Synfony. Mean elastic modulus was in the order of Z250, BelleGlass HP, Tescera, Adoro and Synfony. 3. The result of Vicker's microhardness value showed that significantly higher value in Z250 (p<0.05), and is in the order of BelleGlass HP, Tescera, Adoro and Synfony. 4. The degree of conversion measured by FT-IR showed significantly higher value in BelleGlass HP (p<0.05), and is in the order of Adoro, Synfony, Tescera and Z250. CONCLUSION: Significant differences were found in the flexural strength, wear resistance, hardness and their degree of conversion.
Sujet(s)
Mots clés
Texte intégral: 1 Indice: WPRIM Sujet Principal: Polymères / Vide / Soins dentaires / Module d'élasticité / Polymérisation / Dureté / Température élevée langue: Ko Texte intégral: The Journal of Korean Academy of Prosthodontics Année: 2007 Type: Article
Texte intégral: 1 Indice: WPRIM Sujet Principal: Polymères / Vide / Soins dentaires / Module d'élasticité / Polymérisation / Dureté / Température élevée langue: Ko Texte intégral: The Journal of Korean Academy of Prosthodontics Année: 2007 Type: Article