Surface composition plays an important role in carbon nanotube dispersibility in different environments. Indeed, it determines the choice of dispersion medium. In this paper the effect of oxidation on the dispersion of HiPCO single-walled carbon nanotubes (SWNTs) in N-methyl-pyrrolidinone (NMP), N,N-dimethylformamide (DMF), N,N-dimethylacetamide (DMA), N-dodecyl-pyrrolidinone (N12P) and cyclohexyl-pyrrolidinone (CHP) was systematically studied. During the oxidation process, similar amounts of carboxylic acid and phenolic groups were introduced to mostly already existing defects. For each solvent the dispersion limits and the absorption coefficients were estimated by optical absorption analysis over a range of SWNT concentrations. The presence of acid oxygenated groups increased SWNT dispersibility in NMP, DMF and DMA, but decreased in N12P and CHP. The absorption coefficients, however, decreased for all solvents after oxidation, reflecting the weakening of the effective transition dipole of the π-π transition with even limited extension functionalization and solvent interaction. The analysis of the results in terms of Hansen and Flory-Huggins solubility parameters evidenced the influence of dipolar interactions and hydrogen bonding on the dispersibility of oxidized SWNTs.


Asunto(s)
Amidas/química , Coloides/química , Nanotubos de Carbono/química , Nanotubos de Carbono/ultraestructura , Oxígeno/química , Solventes/química , Sustancias Macromoleculares/química , Ensayo de Materiales , Conformación Molecular , Tamaño de la Partícula , Propiedades de Superficie
SELECCIÓN DE REFERENCIAS
DETALLE DE LA BÚSQUEDA