J Colloid Interface Sci ; 314(2): 510-3, 2007 Oct 15.
Artículo en Inglés | MEDLINE | ID: mdl-17618644

RESUMEN

Sphere- and rod-shaped Zn(2)SiO(4):Mn(2+) phosphor nanocrystals were synthesized at 230 degrees C. The process consists of tuning the surfactant concentration in the oil/surfactant/ethanol system. Powder X-ray (XRD) and transmission electron microscopy (TEM) were used to characterize the phase purity, size and morphology. Photoluminescent (PL) spectra were collected and analyzed. Fourier transform infrared (FT-IR) spectra of the samples indicate the removal of surfactant in the phosphor nanoparticles. As a result, the sphere-shaped phosphor nanoparticles of 100 nm in size can be redispersed in ethanol ultrasonically. The suspension maintain stable for over 48 h.


Asunto(s)
Manganeso/química , Fósforo/química , Silicatos/química , Zinc/química , Etanol/química , Luz , Luminiscencia , Nanopartículas del Metal/química , Microscopía Electrónica de Transmisión , Nanopartículas , Espectrofotometría , Espectroscopía Infrarroja por Transformada de Fourier , Temperatura , Factores de Tiempo , Difracción de Rayos X
SELECCIÓN DE REFERENCIAS
DETALLE DE LA BÚSQUEDA