RESUMEN

BACKGROUND: The blending ability of universal shade composites and their stability in the oral environment are of great concern in restoring anterior teeth. This study aims to evaluate and compare the color stability and surface roughness of two single-shade composite restorations, ormocer-based composite (OBC) and methacrylate resin-based composite (RBC), after storing them in different staining media. MATERIALS AND METHODS: In this study, two universal shade composite restorative materials were tested: a nanohybrid OBC (Admira fusion X-tra, Voco) and a supra-nanofilled RBC (Omnichroma, Toukyama). In total, 60 cylindrical centralized cavities (diameter: 5 mm, depth: 2 mm) were prepared in sound extracted-human central incisors and divided into two equal groups according to the restorative material used (n = 30). According to the storage media, the teeth of each group were divided into three subgroups (n = 10): artificial saliva, black tea, and cola. The restoration color was evaluated for all teeth at baseline and after four weeks of storage. The color stability (∆E) was measured using a reflective spectrophotometer (X-Rite, model RM200QC, Neu-Isenburg, Germany). The surface roughness (Ra) was evaluated using three-dimensional optical profilometry (Wyko, Model NT 1100, Veeco, Tucson, USA). Additionally, the extracted data were analyzed using two-way analysis of variance (ANOVA), one-way ANOVA and Student's t-test. RESULTS: In the baseline evaluation, there were no statistically significant differences with respect to color matching or surface roughness results between the two studied restorative materials. However, the differences were statistically significant after storing them in different media. CONCLUSION: Universal composites showed satisfactory color matching with different teeth colors and accepted surface smoothness, whereas the aging procedure exerted a negative effect on their color stability and surface characteristics.


Asunto(s)
Resinas Compuestas , Restauración Dental Permanente , Color , Materiales Dentales , Restauración Dental Permanente/métodos , Humanos , Ensayo de Materiales , Metacrilatos , Cerámicas Modificadas Orgánicamente , Saliva Artificial , Propiedades de Superficie ,
2.
Braz. dent. sci ; 25(1): 1-8, 2022. tab
Artículo en Inglés | LILACS, BBO | ID: biblio-1354734

RESUMEN

Objective: The present study compared the effect of whitening mouthrinses (WM) on the color change of stained resin composites (RC). Material and Methods: Cylindrical specimens (6mm-diameter and 1mm-thickness) were prepared with the following RC (n=60/group): Filtek Z350XT (Z350- methacrylate-based), Admira Fusion (AD- ormocer-based), TPH3 (TPH- methacrylate-based), and Beautifil II (BII- giomer/methacrylate-based). The initial color was assessed with reflectance spectrophotometer using CIE L*a*b* system. The specimens were immersed in staining broth during 14 days, submitted to color evaluation (ΔE1) and randomly allocated in 4 subgroups (n=15), according to WM adopted: Listerine Whitening (LW-2% hydrogen peroxide), Plax Whitening (PW-1.5% hydrogen peroxide), Bromelain/papain (BP-experimental solution), and Deionized water (DW-negative control). The whitening cycle consisted of RC immersion in WM for 1 min and in artificial saliva for 30 min, simulating 12 weeks, and final color assessment was performed (ΔE2). Color change data were analysed by ANOVA and Tukey's tests (α=5%). Results: After staining, TPH showed the lowest ΔE1 values and Z350 showed the highest color change (p=0.001). The whitening effect promoted by LW was significantly higher than color alteration obtained with PW (ΔE2), and BII showed the highest color change values (ΔE2) after whitening cycle. Conclusion: LW exhibited the greatest whitening potential on stained RC, mainly with the Giomer (Beautifill II) and the Ormocer-based (Admira Fusion) materials. Bromelain/papain solution showed no whitening effect on stained RC. (AU)


Objetivo: O presente estudo comparou o efeito de enxaguatórios clareadores (EC) na alteração de cor de resinas compostas (RC) previamente manchadas. Material e Métodos: Espécimes cilíndricos (6mm de diâmetro e 1mm de espessura) foram preparados com as seguintes RC (n=60/grupo): Filtek Z350XT (Z350- metacrilato), Admira Fusion (AD- ormocer), TPH3 (TPH- metacrilato), e Beautifil II (BII- giomer/metacrilato). A cor inicial foi mensurada com espectrofotômetro de reflectância utilizando o sistema CIE L*a*b*. Os espécimes foram imersos em um caldo de manchamento durante 14 dias, submetidos a avaliação de cor (ΔE1) e alocados aleatoriamente em 4 subgrupos (n=15), de acordo com EC adotado: Listerine Whitening (LW-peróxido de hidrogênio a 2%), Plax Whitening (PW- peróxido de hidrogênio a 1,5%), Bromelina/papaína (BP-solução experimental), e Água deionizada (AD- controle negativo). O ciclo clareador consistiu na imersão da RC no EC por 1 min e na saliva artificial por 30 min, simulando 12 semanas, e a cor final foi mensurada (ΔE2). Os dados de alteração de cor foram analisados pelos testes ANOVA e Tukey (α=5%). Resultados: Após o manchamento, TPH apresentou o menor valor de ΔE1 e Z350 apresentou a maior alteração de cor (p=0,001). O efeito clareador promovido pelo LW foi significativamente maior que o obtido com o PW (ΔE2) e BII teve a maior alteração de cor (ΔE2) após o ciclo clareador. Conclusão: LW exibiu maior potencial clareador nas RC manchadas. BII apresentou maior alteração de cor em resposta à ação clareadora de ambos enxaguatórios à base de peróxido de hidrogênio testados.(AU)


Asunto(s)
Resinas Compuestas , Blanqueadores Dentales , Cerámicas Modificadas Orgánicamente , Peróxido de Hidrógeno
3.
J Contemp Dent Pract ; 22(2): 111-116, 2021 Feb 01.
Artículo en Inglés | MEDLINE | ID: mdl-34257167

RESUMEN

AIM: To compare the color change of three flowable composites after exposure to staining solutions. MATERIALS AND METHODS: A total of 240 oval samples were constructed of conventional flowable resin composite, self-adhesive flowable resin composite, and nanohybrid flowable ormocer (n = 80). Each set was further subcategorized into three subsets as regards staining solution. The baseline color parameters were recorded using spectrophotometer after the immersion of the specimens in artificial saliva for 24 hours. Then, the measurements were taken again after exposure to staining solutions where the color change was measured as ΔE* = V (ΔL*2 + Δa*2 + Δb*2). RESULTS: Conventional flowable resin composite had the best color stability in all staining solutions. The coffee was concluded to be the most staining solution. Compared to beverages, mouthwashes had a greater discoloration effect on nanohybrid flowable ormocer than on selfadhesive flowable composite. CONCLUSION: Conventional flowable composite had the highest color stability among the tested materials, followed by flowable nanohybrid ormocer, and the least was self-adhering flowable composite. Coffee had the greatest discoloration effect, followed by a sports drink and then the energy drink. However, mouthwashes did not have a significant discoloration effect. CLINICAL SIGNIFICANCE: Selection of flowable composite materials that are resistant to staining by coffee, beverages, or mouthwashes is an important factor that may influence the sustainability of the esthetic quality of the restoration.


Asunto(s)
Resinas Compuestas , Materiales Dentales , Café , Color , Ensayo de Materiales , Cerámicas Modificadas Orgánicamente , Espectrofotometría , Propiedades de Superficie
4.
J Prosthodont ; 22(4): 298-303, 2013 Jun.
Artículo en Inglés | MEDLINE | ID: mdl-23387984

RESUMEN

PURPOSE: The purpose of this study was to evaluate the effect of simulated disinfections (2% glutaraldehyde, 1% sodium hypochlorite, and microwave energy) on the surface hardness of Trilux, Biocler, Biotone, New Ace, and Magister commercial artificial teeth. MATERIALS AND METHODS: Specimens (n = 10) were made with the teeth included individually in circular blocks of acrylic resin, leaving the labial surface exposed. Cycles of simulated chemical disinfection were accomplished with the specimens immersed in the solutions at room temperature for 10 minutes, followed by tap water washing for 30 seconds and storage in distilled water at room temperature for 7 days until the next disinfection. Simulated disinfection by microwave energy was carried out in a domestic oven with 1300 W at a potency of 50% for 3 minutes with the specimens individually immersed in 150 ml of distilled water. Control (no disinfection) and the experimental groups (first and third disinfection cycles) were submitted to Knoop hardness measurements with indentations at the center of the labial tooth surface. Data were submitted to repeated measure two-way ANOVA and Tukey's test (α = 0.05). RESULTS: Biocler, Magister, and Trilux showed lower surface microhardness when submitted to microwave. Lower microhardness for Biotone was promoted by hypochlorite, while no significant difference was shown for New Ace. The third disinfection cycle significantly decreased the tooth surface hardness only for microwave. CONCLUSIONS: Different disinfection methods promoted different effects on the microhardness of different types of artificial teeth. Surface microhardness of the teeth was less affected by the simulated chemical disinfections when compared to microwaved specimens.


Asunto(s)
Resinas Acrílicas/química , Desinfectantes Dentales/química , Materiales Dentales/química , Desinfección/métodos , Microondas/uso terapéutico , Diente Artificial , Resinas Acrílicas/efectos de la radiación , Resinas Compuestas/química , Materiales Dentales/efectos de la radiación , Glutaral/química , Dureza , Humanos , Inmersión , Ensayo de Materiales , Cerámicas Modificadas Orgánicamente/química , Polimerizacion , Hipoclorito de Sodio/química , Temperatura , Factores de Tiempo , Agua/química
5.
Gerodontology ; 29(2): e553-9, 2012 Jun.
Artículo en Inglés | MEDLINE | ID: mdl-21787371

RESUMEN

OBJECTIVE: To verify the influence of repeated microwave disinfections on the shear bond strength of two commercial types of teeth to acrylic resin, when the ridge lap surfaces were unmodified, bur abraded, bur grooved or etched by monomer. MATERIAL AND METHODS: Eighty specimens (n = 10) were adhered to the tooth ridge lap surface, polymerised in a water bath at 74°C for 9 h. Microwaved specimens were individually immersed in 150 ml of water and submitted to five simulated disinfections in a microwave oven calibrated at 650 W for 3 min. Control specimens were not microwave treated. Shear bond strength tests were performed in an Instron machine with a cross-speed of 1 mm/min. The fracture load values were transformed into shear bond strength as a function of the bonding area (0.28 cm(2)). Data were submitted to ANOVA and Tukey's test (α = 0.05). Fractured areas were classified as adhesive, cohesive (resin or tooth) or mixed failures. RESULTS: Repeated microwave disinfections increased the shear strength of the tooth/resin bond. Mechanical retention in microwaved and non-microwaved procedures improved the shear bond strength. CONCLUSIONS: The different commercial types of teeth influenced shear bond strength values, with Biotone teeth showing the lower values.


Asunto(s)
Resinas Acrílicas/efectos de la radiación , Recubrimiento Dental Adhesivo , Materiales Dentales/efectos de la radiación , Bases para Dentadura , Desinfección/métodos , Microondas/uso terapéutico , Diente Artificial , Grabado Ácido Dental/métodos , Resinas Acrílicas/química , Adhesividad , Grabado Dental/instrumentación , Materiales Dentales/química , Análisis del Estrés Dental/instrumentación , Humanos , Ensayo de Materiales , Cerámicas Modificadas Orgánicamente/química , Cerámicas Modificadas Orgánicamente/efectos de la radiación , Polimerizacion , Resistencia al Corte , Estrés Mecánico , Propiedades de Superficie , Temperatura , Factores de Tiempo , Agua/química
6.
Dent Mater J ; 28(3): 344-51, 2009 May.
Artículo en Inglés | MEDLINE | ID: mdl-19662734

RESUMEN

In this study, the surface hardness of five light-cured composite resins were evaluated, namely: filled (Estelite), nanofil (AElite), unfilled (Valux Plus), hybrid (Tetric ceram), and Ormocer-based (Admira) composite resins. The microhardness values of composite specimens were measured at the top and bottom surfaces after 24 hours or 30 days of immersion in different solutions (tea, coffee, Turkish coffee, mouthwash, cola, and distilled water). Comparisons were made with univariate analysis of variance and Duncan's multiple range test. It was found that rough specimens of reinforced nano-hybrid composite material immersed in cola for 30 days had the lowest surface hardness (33.20), whereas rough specimens of hybrid composite material immersed in cola for 24 hours had the highest surface hardness (156.00). In both tea and coffee, the top surfaces tended to be harder than the bottom ones. In conclusion, the five different materials exhibited different hardnesses, and that the hardness values of composite materials were statistically different in different immersion solutions.


Asunto(s)
Bebidas , Resinas Compuestas/química , Materiales Dentales/química , Antisépticos Bucales/química , Bebidas Gaseosas , Cerámica/química , Café , Dureza , Humanos , Inmersión , Ensayo de Materiales , Metacrilatos/química , Nanocompuestos/química , Cerámicas Modificadas Orgánicamente , Silanos/química , Siloxanos/química , Soluciones/química , Propiedades de Superficie , , Factores de Tiempo , Agua/química
7.
Eur J Esthet Dent ; 2(2): 236-47, 2007.
Artículo en Inglés | MEDLINE | ID: mdl-19655568

RESUMEN

The purpose of this study was to determine the staining potential of glass-ionomer and composite resin restorative materials following immersion in common beverages. Nine tooth-colored restorative materials were used: three glass ionomers (ceramic-reinforced, resin-modified, and conventional) and six composite resins (nanofilled, ormocer-based, flowable ormocer-based, polyacid-modified, microhybrid, and flowable microhybrid). Disk-shaped specimens were prepared and immersed in 37 degrees C distilled water for 24 hours. Over a 2-week period, five specimens of each material were immersed daily in one of three test beverages (coffee, tea, or cola), then stored in distilled water. A control group of five specimens of each material was continuously immersed in distilled water during the test period. Color coefficients (CIE Lab) were measured by a spectrophotometer before and after staining. All materials were susceptible to staining by all test beverages, while distilled water caused no perceptible color change. As determined by ANOVA and Bonferroni tests, there were highly significant differences in the change in color (deltaE) for tested materials in different beverages (P < or = .001). The deltaE was significantly higher for coffee and tea than for cola; the deltaE was significantly higher for the polyacid-modified composite resin than for all other materials. The material with the least amount of color change in coffee and tea was the ceramic-reinforced glass ionomer (deltaE = 12.45 and 10.64, respectively) and in cola was the nanofilled composite resin (deltaE = 1.93).


Asunto(s)
Bebidas , Resinas Compuestas/química , Materiales Dentales/química , Cementos de Ionómero Vítreo/química , Bebidas Gaseosas , Cerámica/química , Café , Color , Compómeros/química , Humanos , Inmersión , Ensayo de Materiales , Nanocompuestos/química , Cerámicas Modificadas Orgánicamente , Cementos de Resina/química , Silanos/química , Espectrofotometría , Propiedades de Superficie , , Temperatura , Factores de Tiempo , Agua/química