Int J Prosthodont ; 30(5): 461­464, 2017.
Artigo em Inglês | MEDLINE | ID: mdl-28806427

RESUMO

PURPOSE: This clinical trial tested bilayered restorations based on ceria-stabilized tetragonal zirconia/alumina frameworks veneered with feldspathic ceramic. MATERIALS AND METHODS: A total of 67 crowns and 40 fixed dental prostheses (FDPs) were luted in 57 patients with self-etching/self-adhesive composite resin cement. Dental status and integrity of restorations were evaluated at 2 weeks, 6 months, and then annually. RESULTS: A total of 66 crowns and 36 FDPs (88% posterior) survived for success rates of 93.4% for crowns and 89% for FDPs at 2 years. In particular, 11 cohesive ceramic chippings were observed in 5 crowns and 6 FDPs. CONCLUSION: The material allows excellent marginal adaptation. Susceptibility to veneering failures might be due to framework design and the necessities of esthetics.


Assuntos
Óxido de Alumínio , Cério , Prótese Dentária , Nanocompostos , Zircônio , Coroas , Feminino , Humanos , Masculino , Pessoa de Meia-Idade , Desenho de Prótese , Fatores de Tempo , Resultado do Tratamento
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA