Your browser doesn't support javascript.
loading
Mostrar: 20 | 50 | 100
Resultados 1 - 2 de 2
Filtrar
Más filtros

Banco de datos
Tipo del documento
Asunto de la revista
País de afiliación
Intervalo de año de publicación
1.
Nat Commun ; 14(1): 7539, 2023 Nov 20.
Artículo en Inglés | MEDLINE | ID: mdl-37985765

RESUMEN

The rapid diagnosis of respiratory virus infection through breath and blow remains challenging. Here we develop a wireless, battery-free, multifunctional pathogenic infection diagnosis system (PIDS) for diagnosing SARS-CoV-2 infection and symptom severity by blow and breath within 110 s and 350 s, respectively. The accuracies reach to 100% and 92% for evaluating the infection and symptom severity of 42 participants, respectively. PIDS realizes simultaneous gaseous sample collection, biomarker identification, abnormal physical signs recording and machine learning analysis. We transform PIDS into other miniaturized wearable or portable electronic platforms that may widen the diagnostic modes at home, outdoors and public places. Collectively, we demonstrate a general-purpose technology for rapidly diagnosing respiratory pathogenic infection by breath and blow, alleviating the technical bottleneck of saliva and nasopharyngeal secretions. PIDS may serve as a complementary diagnostic tool for other point-of-care techniques and guide the symptomatic treatment of viral infections.


Asunto(s)
Líquidos Corporales , COVID-19 , Humanos , SARS-CoV-2 , COVID-19/diagnóstico , Manejo de Especímenes , Saliva
2.
Mater Sci Eng C Mater Biol Appl ; 33(8): 5001-7, 2013 Dec 01.
Artículo en Inglés | MEDLINE | ID: mdl-24094217

RESUMEN

A mesoporous hydroxyapatite (HA) coating was prepared on a ß-tricalcium phosphate (ß-TCP) porous scaffold by a sol-gel dip-coating method using the block copolymer Pluronic F127 (EO106PO70EO106) as the template. For application as a bone graft, in vitro cell response and bone-related protein expression of mesoporous HA coated ß-TCP scaffold were investigated, using the non-mesoporous HA coated scaffold as the control group, to evaluate the influence of the mesoporous structure on the biological properties of HA coating. It was found that the increased surface area of the mesoporous HA coating greatly affected the response of MC3T3-E1 osteoblasts and the expression of proteins. An enzyme-linked immunosorbent assay recorded a significantly higher expression of alkaline phosphatase (ALP) and bone sialoprotein (BSP) in the mesoporous group than those in the control group (*p<0.05) after different incubation periods. The introduction of mesopores enhanced the expression of ALP and BSP in the cells grown on the mesoporous HA coatings, on the premise of maintaining the protein expression in a sequence to ensure the correct temporo-spatial expression in osteogenesis. These results indicated that the mesoporous HA coating would provide a good environment for cell growth, suggesting that it could be used as the coating material for the surface modification of the tissue engineering scaffolds.


Asunto(s)
Fosfatos de Calcio/química , Durapatita/química , Fosfatasa Alcalina/metabolismo , Animales , Línea Celular , Proliferación Celular/efectos de los fármacos , Materiales Biocompatibles Revestidos/química , Materiales Biocompatibles Revestidos/farmacología , Sialoproteína de Unión a Integrina/metabolismo , Ratones , Osteoblastos/citología , Osteoblastos/efectos de los fármacos , Osteoblastos/metabolismo , Poloxámero/química , Porosidad