INTRODUCTION: Calcium silicate-based materials (CSMs) are used in various endodontic procedures. The present study examined whether prolonged contact of mineralized dentin with recently commercialized versions of these materials adversely affects dentin collagen matrix integrity. METHODS: Dentin slabs prepared from extracted human third molars (7 × 3 × 0.3 mm) were divided into 3 groups on the basis of the material to which dentin was exposed (MTA Plus, Biodentine, untreated control dentin slabs) and the time period of exposure (24 hours, 1, 2, and 3 months; n = 6). Hydroxyproline assay was performed on each group's supernatant to quantify the collagen extraction amounts of each group per time period. Data were analyzed with two-factor repeated-measures analysis of variance and Holm-Sidak pair-wise comparisons (α = 0.05) to determine the effects of material and aging time on collagen extraction. Dentin slabs from the 3 months of aging group were demineralized for transmission electron microscopy examination of collagen matrix ultrastructural changes. RESULTS: Material (P = .002), aging time (P < .001), and their interactions (P = .007) significantly affected the amount of hydroxyproline (pg/mg of mineralized dentin) extracted from mineralized dentin and were significantly correlated by power regression models. Collagen degradation was identified from the surface of dentin slabs that were in direct contact with CSMs. CONCLUSIONS: Prolonged contact of mineralized dentin with CSMs has an adverse effect on the integrity of the dentin collagen matrix. However, the amount of collagen extracted was limited to the contact surface. Clinicians can continue to apply CSMs in endodontic procedures; however, caution is advised when these materials are applied to thin dentinal walls.


Asunto(s)
Compuestos de Calcio/efectos adversos , Colágeno Tipo I/análisis , Dentina/efectos de los fármacos , Matriz Extracelular/efectos de los fármacos , Materiales de Recubrimiento Pulpar y Pulpectomía/efectos adversos , Silicatos/efectos adversos , Compuestos de Aluminio/efectos adversos , Análisis de Varianza , Colágeno Tipo I/efectos de los fármacos , Dentina/química , Combinación de Medicamentos , Matriz Extracelular/química , Humanos , Hidroxiprolina/análisis , Microscopía Electrónica de Transmisión , Óxidos/efectos adversos , Proteolisis , Análisis de Regresión , Materiales de Obturación del Conducto Radicular/efectos adversos , Factores de Tiempo
2.
J Endod ; 38(5): 680-3, 2012 May.
Artículo en Inglés | MEDLINE | ID: mdl-22515902

RESUMEN

INTRODUCTION: Prolonged exposure of root dentin to calcium hydroxide alters the fracture resistance of dentin. Calcium silicate-based materials (CSMs) used in endodontics release calcium hydroxide on setting. This study examined whether prolonged contact of dentin with CSMs adversely affects its mechanical properties. METHODS: Dentin beams prepared from extracted human molars (7 × 3 × 0.3 mm) were divided into 3 groups on the basis of the material to which dentin was exposed (Biodentine, MTA Plus, and untreated control beams). Three-point flexure to failure was performed for each beam at designated exposure times (24 hours, 1, 2, and 3 months; n = 10). Data were analyzed with 2-factor repeated-measures analyses of variance to determine the effects of material and aging time on flexural modulus, flexural strength, and modulus of toughness (α = 0.05). RESULTS: For flexural modulus, there was no significant difference for material (P = .947) or aging time (P = .064) when compared with baseline control. For flexural strength, significant differences were associated with aging time (P < .001) but not with material (P = .349). Flexural strength of dentin exposed to Biodentine decreased significantly after 2 and 3 months, whereas that exposed to MTA Plus decreased significantly after 3 months of aging (P < .05). For modulus of toughness, significant declines were observed for both material (P < .004) and aging time (P < .001). CONCLUSIONS: Both CSMs alter material toughness more than the strength and stiffness of dentin after aging in 100% relative humidity. Because dentin toughness is attributed to its collagen matrix, the amount of collagen extracted from mineralized dentin and changes in collagen ultrastructure should be further examined after exposure of dentin to CSMs.


Asunto(s)
Compuestos de Calcio/farmacología , Dentina/efectos de los fármacos , Materiales de Obturación del Conducto Radicular/farmacología , Silicatos/farmacología , Adolescente , Adulto , Compuestos de Aluminio/farmacología , Fenómenos Biomecánicos , Hidróxido de Calcio/farmacología , Análisis del Estrés Dental/instrumentación , Combinación de Medicamentos , Módulo de Elasticidad , Humanos , Humedad , Ensayo de Materiales , Óxidos/farmacología , Docilidad , Estrés Mecánico , Factores de Tiempo , Adulto Joven