RESUMO
The present work seeks to evaluate the biocompatibility of experimental glass ionomer cements (GIC) prepared from niobium-calcium fluoro-alumino-silicate glass powder and two commercial GICs. The GICs were implanted into the subcutaneous connective tissue of sixty rats. The rats were sacrificed during four varying time periods: 7, 15, 30, and 60 days and histopathological examinations were then performed. The Kruskal-Wallis test was performed to evaluate any significant differences between the materials. Additionally, multiple comparisons of the mean rank were also carried out using the Dunn test (p<0.05). No significant differences were observed that one GIC was superior to the other. The tissue response for all of the GICs tested was similar in all the periods examined.