Waste Manag Res ; 35(2): 181-189, 2017 Feb.
Artigo em Inglês | MEDLINE | ID: mdl-27515667

RESUMO

The pyrolytic characteristics of tyre powder treated under different microwave powers (300, 500, and 700 W) were studied via microwave thermogravimetric analysis. The product yields at different power levels were studied, along with comparative analysis of microwave pyrolysis and conventional pyrolysis. The feedstock underwent preheating, intense pyrolysis, and final pyrolysis in sequence. The main and secondary weight loss peaks observed during the intense pyrolysis stage were attributed to the decomposition of natural rubbers and synthetic rubbers, respectively. The total mass loss rates, bulk temperatures, and maximum temperatures were distinctively higher at higher powers. However, the maximum mass loss rate (0.005 s-1), the highest yields of liquid product (53%), and the minimum yields of residual solid samples (43.83%) were obtained at 500 W. Compared with conventional pyrolysis, microwave pyrolysis exhibited significantly different behaviour with faster reaction rates, which can decrease the decomposition temperatures of both natural and synthetic rubber by approximately 110 °C-140 °C.


Assuntos
Temperatura Alta , Micro-Ondas , Eliminação de Resíduos , Borracha , Termogravimetria/métodos , Resíduos , Desenho de Equipamento , Pós , Termogravimetria/instrumentação , Resíduos/análise
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA