Shear Bond Strength and Adhesive Remnant of Three Protocols used for Bonding Orthodontic Brackets
Morais, Juliana Fernandes de; Chaves, Letícia Virgínia de Freitas; Chaves, Vanessa Suzana de Freitas; Costa, Geórgia Paiva de Faria; Santos, Alex José Sousa; Gadé Neto, Cícero Romão; Machado, Claudia Tavares.
Afiliação
  • Morais, Juliana Fernandes de; Potiguar University. Natal. BR
  • Chaves, Letícia Virgínia de Freitas; s.af
  • Chaves, Vanessa Suzana de Freitas; s.af
  • Costa, Geórgia Paiva de Faria; s.af
  • Santos, Alex José Sousa; Potiguar University. Natal. BR
  • Gadé Neto, Cícero Romão; Potiguar University. Natal. BR
  • Machado, Claudia Tavares; Potiguar University. Natal. BR
Pesqui. bras. odontopediatria clín. integr ; 16(1): 433-440, jan.-dez. 2016. tab, ilus
Article em En | LILACS, BBO | ID: biblio-912895
Biblioteca responsável: BR1822.9
ABSTRACT

Objective:

To test the shear bond strength and the amount of adhesive remnant on the enamel after debonding of a conventional orthodontic composite system, a flowable composite resin, and a self-adhesive resin cement. Material and

Methods:

Thirty extracted bovine incisors were allocated in three groups, according to the type of adhesive Group XT (Transbond XT), Group FL (Flow Z350), and Group RX (RelyX U100). All groups had etching with phosphoric acid. Groups XT and FL received primer before adhesive. Stainless steel metal brackets were bonded using the respective adhesive. Teeth were submitted to shear bond strength (SBS) test, followed by measurement of adhesive remnant. Intergroup comparison of SBS values were performed by one-way Anova and Tukey post-hoc test. Kruskal-Wallis test and the Mann-Whitney U-test were used to compare adhesive remnant.

Results:

Transbond XT presented higher bond strength than RelyX U100 and Flow Z350; all adhesives exhibited bond failure within the adhesive. All groups showed bond failure occurring within the adhesive. Transbond XT and RelyX U100 left significantly more adhesive remnant on the tooth surface than Flow Z350.

Conclusion:

All three adhesive systems had bond strength above the minimum for clinical routine use. As regards to bond strength, Transbond XT performed better than the resin cement and the flowable resin. Bond failure occurred within the adhesive in all groups.
Assuntos
Palavras-chave

Texto completo: 1 Base de dados: BBO / LILACS Assunto principal: Ortodontia / Resinas Compostas / Cimentos Dentários / Resistência ao Cisalhamento Tipo de estudo: Guideline Limite: Animals País/Região como assunto: America do sul / Brasil Idioma: En Revista: Pesqui. bras. odontopediatria clín. integr Assunto da revista: ODONTOLOGIA Ano de publicação: 2016 Tipo de documento: Article País de afiliação: Brasil

Texto completo: 1 Base de dados: BBO / LILACS Assunto principal: Ortodontia / Resinas Compostas / Cimentos Dentários / Resistência ao Cisalhamento Tipo de estudo: Guideline Limite: Animals País/Região como assunto: America do sul / Brasil Idioma: En Revista: Pesqui. bras. odontopediatria clín. integr Assunto da revista: ODONTOLOGIA Ano de publicação: 2016 Tipo de documento: Article País de afiliação: Brasil