1.
Biomaterials ; 24(6): 907-13, 2003 Mar.
Artículo en Inglés | MEDLINE | ID: mdl-12504511

RESUMEN

Solutions of poly(ethylene-co-vinyl alcohol) or EVOH, ranging in composition from 56 to 71 wt% vinyl alcohol, can be readily electrospun at room temperature from solutions in 70% 2-propanol/water (rubbing alcohol). The solutions are prepared at 80 degrees C and allowed to cool to room temperature. Interestingly, the solutions are not stable at room temperature and eventually the polymer precipitates after several hours. However, prior to precipitation, electrospinning is extensive and rapid, allowing coverage of fibers on various substrates, including a grounded metal plate, dielectrics interposed between the charged jet and the metal ground, and on the human body. Fiber diameters of ca. 0.2-8.0 microm were obtained depending upon the solution concentration, an attractive range for tissue engineering, wound healing, and related applications. Electrospun EVOH mats have been shown to support the culturing of smooth muscle cells and fibroblasts.


Asunto(s)
Materiales Biocompatibles/química , Polivinilos/química , 2-Propanol , Animales , Materiales Biocompatibles/farmacología , Células Cultivadas , Fibroblastos/efectos de los fármacos , Fibroblastos/ultraestructura , Mano , Humanos , Microscopía Electrónica de Rastreo/métodos , Músculo Liso/efectos de los fármacos , Músculo Liso/ultraestructura , Nanotecnología/instrumentación , Nanotecnología/métodos , Polivinilos/farmacología , Soluciones , Temperatura , Agua
SELECCIÓN DE REFERENCIAS
DETALLE DE LA BÚSQUEDA