Your browser doesn't support javascript.
loading
Highly Stable Organic Molecular Porous Solid Electrolyte with One-Dimensional Ion Migration Channel for Solid-State Lithium-Oxygen Battery.
Li, Jia-Xin; Guan, De-Hui; Wang, Xiao-Xue; Miao, Cheng-Lin; Li, Jian-You; Xu, Ji-Jing.
Afiliación
  • Li JX; State Key Laboratory of Inorganic Synthesis and Preparative Chemistry, College of Chemistry, Jilin University, Changchun, 130012, P. R. China.
  • Guan DH; State Key Laboratory of Inorganic Synthesis and Preparative Chemistry, College of Chemistry, Jilin University, Changchun, 130012, P. R. China.
  • Wang XX; State Key Laboratory of Inorganic Synthesis and Preparative Chemistry, College of Chemistry, Jilin University, Changchun, 130012, P. R. China.
  • Miao CL; International Center of Future Science, Jilin University, Changchun, 130012, P. R. China.
  • Li JY; State Key Laboratory of Inorganic Synthesis and Preparative Chemistry, College of Chemistry, Jilin University, Changchun, 130012, P. R. China.
  • Xu JJ; International Center of Future Science, Jilin University, Changchun, 130012, P. R. China.
Adv Mater ; 36(23): e2312661, 2024 Jun.
Article en En | MEDLINE | ID: mdl-38290062
ABSTRACT
Solid-state lithium-oxygen (Li-O2) batteries have been widely recognized as one of the candidates for the next-generation of energy storage batteries. However, the development of solid-state Li-O2 batteries has been hindered by the lack of solid-state electrolyte (SSE) with high ionic conductivity at room temperature, high Li+ transference number, and the high stability to air. Herein, the organic molecular porous solid cucurbit[7]uril (CB[7]) with one-dimensional (1D) ion migration channels is developed as the SSE for solid-state Li-O2 batteries. Taking advantage of the 1D ion migration channel for Li+ conduction, CB[7] SSE achieves high ionic conductivity (2.45 × 10-4 S cm-1 at 25 °C). Moreover, the noncovalent interactions facilitated the immobilization of anions, realizing a high Li+ transference number (tLi + = 0.81) and Li+ uniform distribution. The CB[7] SSE also shows a wide electrochemical stability window of 0-4.65 V and high thermal stability and chemical stability, as well as realizes stable Li+ plating/stripping (more than 1000 h at 0.3 mA cm-2). As a result, the CB[7] SSE endows solid-state Li-O2 batteries with superior rate capability and long-term discharge/charge stability (up to 500 h). This design strategy of CB[7] SSE paves the way for stable and efficient solid-state Li-O2 batteries toward practical applications.