Your browser doesn't support javascript.
loading
Dual-cured adhesive system improves adhesive properties of dentin cavities restored with a bulk-fill resin composite
Melo, Ana Margarida dos Santos; Ribeiro, Anne Kaline Claudino; Cunha, Diana Araújo; Rodrigues, Nara Sousa; Saboia, Vicente de Paulo Aragão; Borges, Boniek Castillo Dutra; Assunção, Isauremi Vieira de.
Afiliação
  • Melo, Ana Margarida dos Santos; Universidade Federal do Rio Grande do Norte. Department of Dentistry. Natal. BR
  • Ribeiro, Anne Kaline Claudino; Universidade Federal do Rio Grande do Norte. Department of Dentistry. Natal. BR
  • Cunha, Diana Araújo; Universidade Federal do Ceará. School of Dentistry - Facult of Pharmacy, Dentistry and Nurse. Department of Restorative Dentistry. Fortaleza. BR
  • Rodrigues, Nara Sousa; Universidade Federal do Ceará. School of Dentistry - Facult of Pharmacy, Dentistry and Nurse. Department of Restorative Dentistry. Fortaleza. BR
  • Saboia, Vicente de Paulo Aragão; Universidade Federal do Ceará. School of Dentistry - Facult of Pharmacy, Dentistry and Nurse. Department of Restorative Dentistry. Fortaleza. BR
  • Borges, Boniek Castillo Dutra; Universidade Federal do Rio Grande do Norte. Department of Dentistry. Natal. BR
  • Assunção, Isauremi Vieira de; Universidade Federal do Rio Grande do Norte. Department of Dentistry. Natal. BR
Braz. j. oral sci ; 21: e226262, jan.-dez. 2022. ilus
Article em En | LILACS, BBO | ID: biblio-1354997
Biblioteca responsável: BR218.1
ABSTRACT

Aim:

To evaluate the impact of a dual-cured adhesive system on the in situ degree of conversion (DC), bond strength (BS) and failure mode (FM) of adhesive interfaces in dentin cavities restored with a bulk-fill resin composite.

Methods:

4-mm-deep dentin cavities with a 3.1 C-factor were created in 68 bovine incisors (n = 17 per group). The lightcured (Scotchbond™ Universal) or the dual-cured (Adper™ Scotchbond™ Multi-purpose Plus) adhesive system was applied to the cavities, which were then restored with a bulkfill resin composite (Filtek™ Bulk Fill). In situ DC analysis was performed by means of micro Raman spectroscopy at the top and bottom interfaces. Push-out BS was measured in a universal testing machine after 24-h or 6-month water storage. FM was determined with a stereomicroscope. Data of in situ DC and BS were analyzed by two-way analysis of variance (ANOVA) and Tukey test (p<0.05), while the FM was analyzed descriptively.

Results:

The groups that received the dual-cured adhesive system showed statistically higher in situ DC and BS than those that received the light-cured adhesive system. Cohesive failure mode was the most frequent in all conditions.

Conclusion:

In situ DC and BS were influenced by the curing strategies of the adhesive systems with better performance of the dual-cured

material:

Assuntos
Palavras-chave

Texto completo: 1 Base de dados: BBO / LILACS Assunto principal: Envelhecimento / Adesivos Dentinários / Resinas Compostas / Polimerização Idioma: En Ano de publicação: 2022 Tipo de documento: Article País de afiliação: Brasil

Texto completo: 1 Base de dados: BBO / LILACS Assunto principal: Envelhecimento / Adesivos Dentinários / Resinas Compostas / Polimerização Idioma: En Ano de publicação: 2022 Tipo de documento: Article País de afiliação: Brasil