Dent Mater J ; 34(5): 618-22, 2015.
Article in English | MEDLINE | ID: mdl-26438985

ABSTRACT

The aim was to evaluate the effects of fiber-reinforced composite restorations and a bulk-fill resin composite on the fracture strength of mandibular premolars treated endodontically. Standard mesio-occluso-distal (MOD) cavities were prepared in 48 mandibular premolars. Following root canal treatment, teeth were assigned to four groups: Group 1, nano-hybrid resin composite; Group 2, polyethylene woven fiber plus nano-hybrid resin composite; Group 3, short fiber-reinforced resin composite plus nano-hybrid resin composite; and Group 4, bulk-fill resin composite plus nano-hybrid resin composite. Then, the teeth were subjected to the fracture toughness test. The data were analyzed statistically using one-way ANOVA, followed by Tukey's post-hoc test. The fiber-reinforced groups had better results than the nano-hybrid and bulk-fill composites (p<0.05), while the bulk-fill and nano-hybrid composite restorations gave similar results (p>0.05). Fiber-reinforcement improved the fracture strength of teeth with large MOD cavities treated endodontically. Bulk-fill composites can be used reliably as well as nano-hybrid composites.


Subject(s)
Composite Resins/chemistry , Dental Restoration, Permanent/methods , Dental Restoration, Permanent/statistics & numerical data , Tooth Fractures/prevention & control , Tooth, Nonvital/surgery , Analysis of Variance , Humans , Polyethylenes/chemistry
SELECTION OF CITATIONS
SEARCH DETAIL
...