ABSTRACT
Cobalt-base alloys (Co-Cr-Mo) are widely employed in dentistry and orthopedic implants due to their biocompatibility, high mechanical strength and wear resistance. The osseointegration of implants can be improved by surface modification techniques. However, complex geometries obtained by additive manufacturing (AM) limits the efficiency of mechanical-based surface modification techniques. Therefore, plasma immersion ion implantation (PIII) is the best alternative, creating nanotopography even in complex structures. In the present study, we report the osseointegration results in three conditions of the additively manufactured Co-Cr-Mo alloy: (i) as-built, (ii) after PIII, and (iii) coated with titanium (Ti) followed by PIII. The metallic samples were designed with a solid half and a porous half to observe the bone ingrowth in different surfaces. Our results revealed that all conditions presented cortical bone formation. The titanium-coated sample exhibited the best biomechanical results, which was attributed to the higher bone ingrowth percentage with almost all medullary canals filled with neoformed bone and the pores of the implant filled and surrounded by bone ingrowth. It was concluded that the metal alloys produced for AM are biocompatible and stimulate bone neoformation, especially when the Co-28Cr-6Mo alloy with a Ti-coated surface, nanostructured and anodized by PIII is used, whose technology has been shown to increase the osseointegration capacity of this implant.
ABSTRACT
This work evaluated the effects of UV irradiation, plasma radiation, steam and 70% ethanol treatments on the sterilization and integrity of auto-crosslinked hyaluronic acid (HA-ACP) scaffolds structured in microparticles and sponges aiming in vivo applications for regenerative medicine of bone tissue. The integrity of the microparticles was characterized by rheological behavior, while for the sponges, it was characterized by scanning electron microscopy, Fourier transform infrared spectroscopy and differential scanning calorimetry. The effectiveness of the sterilization treatment was verified by the number of microorganism colonies in the samples after the treatments. In conclusion, plasma radiation was the best treatment for the sponges, while steam sterilization in the autoclave at 126°C (1.5 kgf/cm2) for 5 min was the best treatment for the microparticles.
Subject(s)
Disinfection/methods , Hyaluronic Acid/chemistry , Nanoparticles/chemistry , Sterilization/methods , Tissue Scaffolds/chemistry , Bone and Bones , Calorimetry, Differential Scanning , Chemical Phenomena , Ethanol/pharmacology , Microscopy, Electron, Scanning , Microspheres , Nanoparticles/microbiology , Radiation , Spectroscopy, Fourier Transform Infrared , Tissue Engineering , Tissue Scaffolds/microbiology , Ultraviolet RaysABSTRACT
PURPOSE: To investigate the osseointegration properties of prototyped implants with tridimensionally interconnected pores made of the Ti6Al4V alloy and the influence of a thin calcium phosphate coating. METHODS: Bilateral critical size calvarial defects were created in thirty Wistar rats and filled with coated and uncoated implants in a randomized fashion. The animals were kept for 15, 45 and 90 days. Implant mechanical integration was evaluated with a push-out test. Bone-implant interface was analyzed using scanning electron microscopy. RESULTS: The maximum force to produce initial displacement of the implants increased during the study period, reaching values around 100N for both types of implants. Intimate contact between bone and implant was present, with progressive bone growth into the pores. No significant differences were seen between coated and uncoated implants. CONCLUSION: Adequate osseointegration can be achieved in calvarial reconstructions using prototyped Ti6Al4V Implants with the described characteristics of surface and porosity.
Subject(s)
Ceramics/therapeutic use , Implants, Experimental , Osseointegration/physiology , Skull/surgery , Titanium/therapeutic use , Animals , Calcium Phosphates , Ceramics/chemistry , Coated Materials, Biocompatible , Male , Materials Testing , Microscopy, Electron, Scanning , Rats, Wistar , Reproducibility of Results , Spectrometry, X-Ray Emission , Surface Properties , Time Factors , Titanium/chemistry , Treatment OutcomeABSTRACT
Additive manufacturing (AM) technology from engineering has helped to achieve several advances in the medical field, particularly as far as fabrication of implants is concerned. The use of AM has made it possible to carry out surgical planning and simulation using a three-dimensional physical model which accurately represents the patient's anatomy. AM technology enables the production of models and implants directly from a 3D virtual model, facilitating surgical procedures and reducing risks. Furthermore, AM has been used to produce implants designed for individual patients in areas of medicine such as craniomaxillofacial surgery, with optimal size, shape and mechanical properties. This work presents AM technologies which were applied to design and fabricate a biomodel and customized implant for the surgical reconstruction of a large cranial defect. A series of computed tomography data was obtained and software was used to extract the cranial geometry. The protocol presented was used to create an anatomic biomodel of the bone defect for surgical planning and, finally, the design and manufacture of the patient-specific implant.
Subject(s)
Computer-Aided Design , Imaging, Three-Dimensional/methods , Models, Anatomic , Plastic Surgery Procedures/methods , Prostheses and Implants , Prosthesis Design , Skull/surgery , Alloys/chemistry , Biocompatible Materials/chemistry , Biomedical Engineering , Biomedical Technology , Computer Simulation , Decompressive Craniectomy/adverse effects , Frontal Bone/injuries , Frontal Bone/surgery , Humans , Image Processing, Computer-Assisted/methods , Male , Patient Care Planning , Printing, Three-Dimensional , Software , Surgery, Computer-Assisted , Titanium/chemistry , Tomography, X-Ray Computed/methods , User-Computer Interface , Young AdultABSTRACT
PURPOSE: To investigate the osseointegration properties of prototyped implants with tridimensionally interconnected pores made of the Ti6Al4V alloy and the influence of a thin calcium phosphate coating. METHODS: Bilateral critical size calvarial defects were created in thirty Wistar rats and filled with coated and uncoated implants in a randomized fashion. The animals were kept for 15, 45 and 90 days. Implant mechanical integration was evaluated with a push-out test. Bone-implant interface was analyzed using scanning electron microscopy. RESULTS: The maximum force to produce initial displacement of the implants increased during the study period, reaching values around 100N for both types of implants. Intimate contact between bone and implant was present, with progressive bone growth into the pores. No significant differences were seen between coated and uncoated implants. CONCLUSION: Adequate osseointegration can be achieved in calvarial reconstructions using prototyped Ti6Al4V Implants with the described characteristics of surface and porosity. .
Subject(s)
Animals , Male , Ceramics/therapeutic use , Implants, Experimental , Osseointegration/physiology , Skull/surgery , Titanium/therapeutic use , Calcium Phosphates , Coated Materials, Biocompatible , Ceramics/chemistry , Materials Testing , Microscopy, Electron, Scanning , Rats, Wistar , Reproducibility of Results , Spectrometry, X-Ray Emission , Surface Properties , Time Factors , Treatment Outcome , Titanium/chemistryABSTRACT
PURPOSE:To investigate the osseointegration properties of prototyped implants with tridimensionally interconnected pores made of the Ti6Al4V alloy and the influence of a thin calcium phosphate coating.METHODS:Bilateral critical size calvarial defects were created in thirty Wistar rats and filled with coated and uncoated implants in a randomized fashion. The animals were kept for 15, 45 and 90 days. Implant mechanical integration was evaluated with a push-out test. Bone-implant interface was analyzed using scanning electron microscopy.RESULTS:The maximum force to produce initial displacement of the implants increased during the study period, reaching values around 100N for both types of implants. Intimate contact between bone and implant was present, with progressive bone growth into the pores. No significant differences were seen between coated and uncoated implants.CONCLUSION:Adequate osseointegration can be achieved in calvarial reconstructions using prototyped Ti6Al4V Implants with the described characteristics of surface and porosity.(AU)