ABSTRACT

PURPOSE: To investigate the effect of different light-curing units and depths on the degree of conversion (DC) through Fourier transform infrared spectroscopy (FTIR) and Knoop Hardness Number (KHN) of a silorane-based composite resin (Filtek LS, 3M ESPE, St Paul, MN, USA) (LS). MATERIALS AND METHODS: LS specimens mounted in a particular designed matrix were photoactivated by three light-cure units (LCUs) at depths of 2, 3, 4, and 5 mm. The DC was determined in a FTIR spectrometer with an attenuated total reflectance accessory. The KHN was measured in an automatic microhardness tester. The results were analyzed using the Friedman and Spearman statistical tests (α=0.05). RESULTS: There was no effect of LCUs on the DC (p=0.472) or KHN (p=0.174) for all of the studied depths. The highest DC and KHN means were found at 2-mm depth, which were not statistically different from 3-mm depth, but were higher than 4-mm and 5-mm depths (p=0.007). Spearman analysis found a positive linear correlation between the variables KHN and DC (r=0.858, p<0.000). CONCLUSIONS: The LCUs' effect was not verified. Values of DC and KHN for LS decreased with increasing depth. The highest values for both DC and KHN were obtained at depths of 2-3 mm.


Subject(s)
Composite Resins/therapeutic use , Light-Curing of Dental Adhesives/methods , Dental Restoration, Permanent/methods , Dental Stress Analysis , Hardness , Humans , Spectroscopy, Fourier Transform Infrared
SELECTION OF CITATIONS
SEARCH DETAIL
...