1.
Int J Immunopathol Pharmacol ; 36: 3946320221125090, 2022.
Artículo en Inglés | MEDLINE | ID: mdl-36121435

RESUMEN

Burn healing should be regarded as a dynamic process consisting of two main, interrelated phases: (a) the inflammatory phase when neutrophils and monocytes infiltrate the injury site, through localized vasodilation and fluid extravasation, and (b) the proliferative-remodeling phase, which represents a key event in wound healing. In the skin, both canonical autophagy (induced by starvation, oxidative stress, and environmental aggressions) and non-canonical or selective autophagy have evolved to play a discrete, but, essential, "housekeeping" role, for homeostasis, immune tolerance, and survival. Experimental data supporting the pro-survival roles of autophagy, highlighting its Yang, luminous and positive feature of this complex but insufficient explored molecular pathway, have been reported. Autophagic cell death describes an "excessive" degradation of important cellular components that are necessary for normal cell function. This deadly molecular mechanism brings to light the darker, concealed, Yin feature of autophagy. Autophagy seems to perform dual, conflicting roles in the angiogenesis context, revealing once again, its Yin-Yang features. Autophagy with its Yin-Yang features remains the shadow player, able to decide quietly whether the cell survives or dies.


Asunto(s)
Autofagia , Quemaduras , Homeostasis , Humanos , Estrés Oxidativo , Cicatrización de Heridas
2.
Materials (Basel) ; 15(9)2022 Apr 23.
Artículo en Inglés | MEDLINE | ID: mdl-35591410

RESUMEN

A provisionalization sequence is essential for obtaining a predictable final prosthetic outcome. An assessment of the mechanical behavior of interim prosthetic materials could orient clinicians towards selecting an appropriate material for each clinical case. The aim of this study was to comparatively evaluate the mechanical behavior-with compressive and three-point flexural tests-of certain 3D-printed and conventional resins used to obtain interim fixed dental prostheses. Four interim resin materials were investigated: two 3D-printed resins and two conventional resins (an auto-polymerized resin and a pressure/heat-cured acrylic resin). Cylindrically shaped samples (25 × 25 mm/diameter × height) were obtained for the compression tests and bar-shaped samples (80 × 20 × 5 mm/length × width × thickness) were produced for the flexural tests, observing the producers' recommendations. The resulting 40 resin samples were subjected to mechanical tests using a universal testing machine. Additionally, a fractographic analysis of failed samples in bending was performed. The results showed that the additive manufactured samples exhibited higher elastic moduli (2.4 ± 0.02 GPa and 2.6 ± 0.18 GPa) than the conventional samples (1.3 ± 0.19 GPa and 1.3 ± 0.38 GPa), as well as a higher average bending strength (141 ± 17 MPa and 143 ± 15 MPa) when compared to the conventional samples (88 ± 10 MPa and 76 ± 7 MPa); the results also suggested that the materials were more homogenous when produced via additive manufacturing.

3.
Materials (Basel) ; 14(22)2021 Nov 15.
Artículo en Inglés | MEDLINE | ID: mdl-34832293

RESUMEN

The fabrication of fixed dental prostheses using aesthetic materials has become routine in today's dentistry. In the present study, three-unit full zirconia fixed prosthetic restorations obtained by computer-aided design/computer-aided manufacturing (CAD/CAM) technology were tested by bending trials. The prostheses were intended to replace the first mandibular left molar and were manufactured from four different types of zirconia bioceramics (KatanaTM Zirconia HTML and KatanaTM Zirconia STML/Kuraray Noritake Dental Inc.; NOVAZir® Fusion float® ml/NOVADENT/Dentaltechnik; and 3D PRO Zirconia/Bloomden Bioceramics). In total, sixteen samples were manufactured-four samples per zirconia material. Additionally, the morphology, grain size area distribution, and elemental composition were analyzed in parallelepiped samples made from the selected types of zirconia in three different areas, noted as the upper, middle, and lower areas. The scanning electron microscope (SEM) analysis highlighted that the grain size area varies with respect to the researched area and the type of material. Defects such as microcracks and pores were also noted to a smaller extent. In terms of grain size area, it was observed that most of the particles in all samples were under 0.5 µm2, while the chemical composition of the investigated materials did not vary significantly. The results obtained after performing the bending tests showed that a zirconia material with fewer structural defects and an increased percentage of grain size area under 0.5 µm2, ranging from ~44% in the upper area to ~74% in the lower area, exhibited enhanced mechanical behavior. Overall, the resulting values of all investigated parameters confirm that the tested materials are suitable for clinical use.

4.
Materials (Basel) ; 15(1)2021 Dec 29.
Artículo en Inglés | MEDLINE | ID: mdl-35009373

RESUMEN

The purpose of this study was to analyze the oxidative stress level and inflammatory status of saliva in the presence of certain materials used for obtaining interim prosthetic restorations. Four types of interim resin materials were investigated: a pressure/heat-cured acrylic resin (Superpont C+B, SpofaDental a.s Czech Republic, /KaVo Kerr Group), a milled resin (Telio CAD polymethyl methacrylate, Ivoclar Vivadent AG, Liechtenstein), a 3D printed resin (NextDent C&B MFH, NextDent by 3D Systems, the Netherlands), and a pressure/heat-cured micro-filled indirect composite resin (SR Chromasit, Ivoclar Vivadent AG, Liechtenstein). The disk-shaped resin samples (30 mm diameter, 2 mm high) were obtained in line with the producers' recommendations. The resulting resin specimens were incubated with saliva samples collected from twenty healthy volunteers. In order to analyze the antioxidant activity of the tested materials, certain salivary parameters were evaluated before and after incubation: uric acid, gamma glutamyl transferase (GGT), oxidative stress responsive kinase-1 (OXSR-1), and total antioxidant capacity (TAC); the salivary levels of tumor necrosis factor (TNFα) and interleukin-6 (IL-6) (inflammatory markers) were measured as well. The obtained results are overall favorable, showing that the tested materials did not cause significant changes in the salivary oxidative stress level and did not influence the inflammatory salivary status.