1.
Talanta ; 148: 285-91, 2016.
Artículo en Inglés | MEDLINE | ID: mdl-26653451

RESUMEN

A new diffusive gradients in thin films (DGT) device, using Pb(II) ion-imprinted silica (IIS) as the binding agents and commercial cellulose acetate dialysis (CAD) membrane as the diffusion layer (CAD/IIS-DGT), has been developed and evaluated for sampling and measurement of free Pb(II) species. The CAD/IIS-DGT devices were successfully applied to the measurement of free Pb(II) species in synthetic solutions, in natural freshwaters and in industrial wastewaters. The CAD/IIS-DGT provides reliable results over pH range of 4.5-6.5 and a wide range of ionic strength from 1.0×10(-3) to 0.7 mol L(-1). The concentrations of the free Pb(II) species in synthetic solution containing different concentrations of ligands measured by CAD/IIS-DGT showed a good agreement with the value measured by Pb-ion selective electrode. Field deployments of the CAD/IIS-DGT devices allowed accurate measurements of the concentrations of free Pb(II) species.


Asunto(s)
Plomo/análisis , Impresión Molecular/métodos , Dióxido de Silicio/química , Adsorción , Difusión , Electroforesis en Acetato de Celulosa/métodos
2.
Talanta ; 114: 276-82, 2013 Sep 30.
Artículo en Inglés | MEDLINE | ID: mdl-23953471

RESUMEN

A 0.050 mol L(-1) solution of poly (ethyleneimine) (PEI), had been used as a novel binding agent of diffusive gradients in thin-films (DGT) technique (PEI-DGT) for measuring the concentrations of labile Cu(2+), Cd(2+) and Pb(2+) in waters. The binding capacities of the PEI-DGT for Cu(2+), Cd(2+) and Pb(2+) were 11.8, 10.2 and 10.6 µmol L(-1), respectively. The performance of PEI-DGT was independence of pH in the range of 4-8 and ionic strength in the range from 1×10(-4) to 0.1 mol L(-1) (as NaNO3). PEI-DGT could measure 104.7±5.2% of the total concentration of Cd(2+) (0.500 mg L(-1)), 95.2±4.3% of the total Cu(2+) (0.500 mg L(-1)) and 99.2±3.4% of the total Pb(2+) (0.500 mg L(-1)) in synthetic solution. Effects of the ligands on the measurement of labile metals were also investigated in synthetic solutions containing the various concentrations of EDTA and humic acid. In EDTA solution, the concentrations of labile metals measured by PEI-DGT showed good agreement with the theoretical concentrations of free metal ions. In humic acid solution, the concentrations of labile metals measured by PEI-DGT decreased with the increase of the concentrations of humic acid. Several DGT devices with various binding agents, including PEI, sodium polyacrylate and poly(4-styrenesulfonate) solution, were used for the measurement of labile fractions of Cu(2+), Cd(2+) and Pb(2+) in the spiked waters and in mine wastewaters. The results showed that the concentrations of labile metal measured by DGT devices with different binding agents could be significantly different, indicating that the labile fractions of metals were dependent on the binding strength of the binding agents with metals. By choosing binding agents, the useful information on the speciation and bioavailability of the analytes can be provided.


Asunto(s)
Metales Pesados/análisis , Polietileneimina/química , Contaminantes Químicos del Agua/análisis , Celulosa/análogos & derivados , Celulosa/química , China , Monitoreo del Ambiente , Residuos Industriales , Lagos/química , Membranas Artificiales , Metales Pesados/química , Minería , Ríos/química , Soluciones , Aguas Residuales/análisis , Contaminantes Químicos del Agua/química
3.
J Hazard Mater ; 260: 762-9, 2013 Sep 15.
Artículo en Inglés | MEDLINE | ID: mdl-23856306

RESUMEN

A new diffusive gradients in thin-films (DGT) device with solution of polymer-bound Schiff base (Py-PEI) derived from poly(ethyleneimine) and 2-pyridinecarboxaldehyde as the binding agent (Py-PEI DGT) was developed for measuring labile Cu(2+), Cd(2+) and Pb(2+) in waters. In synthetic solution, uptake percentages of Cu(2+), Cd(2+) and Pb(2+) by Py-PEI DGT were 99.2 ± 4.4%, 103.7 ± 4.8% and 98.7 ± 5.5% of the total metals, respectively. Performance of Py-PEI DGT was independent of pH 4-8.5 and ionic strength 1 × 10(-4)-0.1 mol L(-1). The uptake of labile metals showed agreement with the theoretical values of free ions in EDTA solution, and decreased with increase of humic acid (HA) and dissolved organic carbon (DOC) contents in water due to the complexation of HA and DOC with metals. DGT devices containing different liquid binding agents (Py-PEI, polyacrylate (PA) and poly(4-styrenesulfonate) (PSS)) were deployed in the same solution. The higher uptake percentages of Py-PEI DGT (13.2 ± 1.1, 26.5 ± 2.4 and 62.7 ± 3.2% of total Cu(2+), Cd(2+) and Pb(2+)) were obtained with respective to PSS DGT (6.7 ± 0.6, 9.2 ± 0.9 and 29.6 ± 2.7% of total above metals) and PA DGT (8.9 ± 0.9 and 16.2 ± 1.1% of total Cu(2+) and Cd(2+)) due to its relatively strong binding affinity with metals.


Asunto(s)
Cadmio/química , Cobre/química , Plomo/química , Contaminantes Químicos del Agua/análisis , China , Difusión , Electrólitos , Monitoreo del Ambiente , Concentración de Iones de Hidrógeno , Iones , Ligandos , Membranas Artificiales , Metales/química , Metales Pesados , Polietileneimina/química , Polímeros/química , Piridinas/química , Reproducibilidad de los Resultados , Ríos , Bases de Schiff , Espectroscopía Infrarroja por Transformada de Fourier , Contaminantes Químicos del Agua/química , Purificación del Agua/métodos