RESUMEN

OBJECTIVE: The aim of this study was to evaluate bovine enamel wear opposed to four different ceramic substrates (CEREC) in the glazed and polished conditions. METHOD AND MATERIALS: Sixty-three ceramic (IPS Empress CAD, Paradigm C, Vitablocs Mark II) and fourteen composite resin (MZ100) styli were prepared. Ceramics were subdivided into three surface conditions (n = 7), unpolished, polished, and glazed, and the composite resin (n = 7) into unpolished and polished. All styli were used as wear antagonists opposing bovine enamel blocks (8 mm × 9 mm) in an oral wear simulator. Wear tests were conducted at 30 N abrasion and 70 N attrition forces applied at 1.7 Hz for 5,000 simulated mastication cycles. Abrasion and attrition wear were evaluated using an automatic profilometer. Statistical analyses were conducted using Tukey's B rank order test, P = .05. RESULTS: For bovine enamel opposing glazed Vitablocs, abrasion and attrition wear showed a volume loss significantly higher than bovine enamel opposing polished Vitablocs (P < .05). For attrition wear, bovine enamel opposing glazed Vitablocs and untreated Paradigm C showed a volume loss higher than bovine enamel opposing the other ceramic conditions. CONCLUSION: Abrasion and attrition wear of bovine enamel opposing antagonist ceramic was affected according to the ceramic surface condition and the ceramic material. Antagonistic wear against the studied ceramic materials and conditions exhibited wear rates within the range of normal enamel. In addition, the glaze layer presented as a protection, exhibiting fewer cracks and less loss of material on the ceramic surface.


Asunto(s)
Cerámica , Materiales Dentales , Desgaste de los Dientes , Resinas Compuestas , Humanos , Microscopía Electrónica de Rastreo , Propiedades de Superficie
2.
Acta Odontol Latinoam ; 25(1): 109-14, 2012.
Artículo en Inglés | MEDLINE | ID: mdl-22928390

RESUMEN

This study evaluated the influence of the prolonged setting time of an ethanol-based adhesive system on the dentin bond strength and degree of conversion. Labial and lingual surfaces of fifteen human third molars were flattened until the dentin was exposed and randomly allocated to 3 groups (n = 10), according to the dwell time between the application of two consecutive layers of the adhesive system (Adper Single Bond Plus, 3M ESPE) and light activation: G1--control (no extra dwell time); G2 and G3--dwell time of 30 seconds and 60 seconds, respectively. After light curing, two cylinders (1.4 x 1 mm) of composite resin (Filtek Flow, 3M ESPE) were bonded to each surface and submitted to micro-shear testing, 24 hours after light curing. A similar adhesive procedure was used for the degree of conversion evaluation using Fourier transform infrared spectroscopy (FTIR). Significant differences between bond strength values (p = 0.0003) and degrees of conversion (p = 0.0004) were detected. The bond strength of G3 (60-second dwell time) was statistically higher than that of other groups. G1 (control) and G2 (30-second dwell time) presented similar results. Values of degree of conversion indicated that both the 30-second and 60-second dwell times resulted in similar and greater percentages of conversion. The use of a longer dwell time (60 seconds) might provide better solvent volatilization and monomer infiltration; bringing benefits to dentin bonding using simplified etch & rinse adhesive systems.


Asunto(s)
Recubrimiento Dental Adhesivo , Recubrimientos Dentinarios , Solventes , Resinas Compuestas , Etanol , Humanos , Técnicas In Vitro , Resistencia al Corte , Factores de Tiempo