Mater Today Proc ; 89: 24-29, 2023 Sep 05.
Article En | MEDLINE | ID: mdl-38590583

Studies have reported challenges of debonding of dental zirconia crowns to from luting cement and prepared teeth. The aim of the study was to explore the application of dental glazing systems for enhancing the bonding of zirconia dental ceramics to luting resin cement. Commercial glaze powder and liquid (Vita Akzent) and experimental mica-based glaze powders were used for the study. X-ray diffraction analysis of the glaze powders (XRD) and Fourier Transform InfraRed Spectroscopy (FTIR) was done on the glaze liquid. Sandblasted sintered dental zirconia (Katana, Noritake) were the control samples. Glazed zirconia samples were coated with commercial glaze and experimental glaze powders which were further etched with 5% hydrofluoric acid. Shear bond strengths of sandblasted and glazed zirconia samples to resin composites were evaluated. XRD of commercial and experimental glaze powders revealed a broad peak confirming the amorphous nature of glass and FTIR analysis of the glaze liquid revealed symmetrical stretching (CH2-CH3) of the alcohol group indicating a mixture of iso-butane and ethanol. Glazed and etched zirconia showed significantly higher shear bond strength to resin cement compared to sand-blasted zirconia. The study confirms the glassy nature of dental glaze powders and the presence of ethanol-based mixtures in the commercial glaze liquid. Glazing systems have the potential to be explored for enhancing the bonding of non-etchable zirconia ceramics to resin cement and tooth substrates.

...