Static Behavior of a 3D-Printed Short Carbon Fiber Polyamide: Influence of the Meso-Structure and Water Content.
Canegrati, Andrea; Martulli, Luca Michele; Kostovic, Milutin; Rollo, Gennaro; Sorrentino, Andrea; Carboni, Michele; Bernasconi, Andrea.
Affiliation
  • Canegrati A; Department of Mechanical Engineering, Politecnico di Milano, Via La Masa 1, 20156 Milano, Italy.
  • Martulli LM; Department of Mechanical Engineering, Politecnico di Milano, Via La Masa 1, 20156 Milano, Italy.
  • Kostovic M; Polymer, Composites and Biomaterials Institute, National Research Council (CNR), Via Previati 1/E, 23900 Lecco, Italy.
  • Rollo G; Polymer, Composites and Biomaterials Institute, National Research Council (CNR), Via Previati 1/E, 23900 Lecco, Italy.
  • Sorrentino A; Polymer, Composites and Biomaterials Institute, National Research Council (CNR), Via Previati 1/E, 23900 Lecco, Italy.
  • Carboni M; Department of Mechanical Engineering, Politecnico di Milano, Via La Masa 1, 20156 Milano, Italy.
  • Bernasconi A; Department of Mechanical Engineering, Politecnico di Milano, Via La Masa 1, 20156 Milano, Italy.
Materials (Basel) ; 17(9)2024 Apr 24.
Article in En | MEDLINE | ID: mdl-38730790
ABSTRACT
The knowledge of the mechanical behavior of a 3D-printed material is fundamental for the 3D printing outbreaking technology to be considered for a range of applications. In this framework, the significance, reliability, and accuracy of the information obtained by testing material coupons assumes a pivotal role. The present work focuses on an evaluation of the static mechanical properties and failure modes of a 3D-printed short carbon fiber-reinforced polyamide in relation to the specimen's unique meso-structural morphology and water content. Within the manufacturing limitations of a commercially available printer, specimens of dedicated combinations of geometry and printing patterns were specifically conceived and tested. The specimens' meso-structure morphologies were investigated by micro-computed tomography. The material failure mechanisms were inferred from an analysis of the specimens' fracture surfaces and failure morphologies. The outcomes of the present analysis indicate that each test specimen retained proper mechanical properties, thereby suggesting that they should be accurately designed to deliver representative information of the underlying material beads or of their deposition layout. Suggestions on the adoption of preferred test specimens for evaluating specific material properties were proposed.