Your browser doesn't support javascript.
loading
J-Integral Experimental Reduction Reveals Fracture Toughness Improvements in Thin-Ply Carbon Fiber Laminates with Aligned Carbon Nanotube Interlaminar Reinforcement.
Furtado, Carolina; Kopp, Reed; Ni, Xinchen; Sarrado, Carlos; Kalfon-Cohen, Estelle; Wardle, Brian L; Camanho, Pedro P.
Affiliation
  • Furtado C; DEMec, Faculdade de Engenharia, Universidade do Porto, Rua Dr. Roberto Frias, s/n, Porto 4200-465, Portugal.
  • Kopp R; INEGI, Instituto de Ciência e Inovação em Engenharia Mecânica e Engenharia Industrial, Rua Dr. Roberto Frias, 400, Porto 4200-465, Portugal.
  • Ni X; Department of Aeronautics and Astronautics, Massachusetts Institute of Technology, 77 Massachusetts Avenue, Cambridge, Massachusetts 02139, United States.
  • Sarrado C; Department of Aeronautics and Astronautics, Massachusetts Institute of Technology, 77 Massachusetts Avenue, Cambridge, Massachusetts 02139, United States.
  • Kalfon-Cohen E; Department of Mechanical Engineering, Massachusetts Institute of Technology, 77 Massachusetts Avenue, Cambridge, Massachusetts 02139, United States.
  • Wardle BL; AMADE, Polytechnic School, Universitat de Girona, Campus Montilivi s/n, Girona 17073, Spain.
  • Camanho PP; AMTEC Composites, C/Pic de Peguera 15, Girona 17003, Spain.
Article in En | MEDLINE | ID: mdl-38624137
ABSTRACT
The Mode I, Mode II, and mixed-mode interlaminar failure behavior of a thin-ply (54 gsm) carbon fiber-epoxy laminated composite reinforced by 20 µm tall z-direction-aligned carbon nanotubes (CNTs), comprising ∼50 billion CNT fibers per cm2, is analyzed following J-integral-based data reduction methods. The inclusion of aligned CNTs in the ply interfaces provides enhanced crack resistance, resulting in sustained crack deflection from the reinforced interlaminar region to the intralaminar region of the adjacent plies, i.e., the CNTs drive the crack from the interlaminar region into the plies. The CNTs do not appreciably increase the interlaminar thickness or laminate weight and preserve the intralaminar microfiber morphology. Improvements of 34 and 62% on the Mode I and Mode II initiation fracture toughness, respectively, are observed. This type of interlaminar nanoreinforcement effectively drives crack propagation from the interface to within the ply where the crack propagates parallel to the interlaminar region, providing new insight into previously reported strength and fatigue performance increases. These findings extend to industries where lightweight and durable materials are critical for improving the structural efficiency.