Avaliação da estabilidade dimensional de três marcas de hidrocoloides irreversíveis / Evaluation of the dimensional stability of three irreversible hydrocolloids
Werneck, Rafael Dario; Marba, Luciana; Finck, Nathalia Silveira; Garcia, Isis Morosini; Delai, Paola.
Affiliation
  • Werneck, Rafael Dario; s.af
  • Marba, Luciana; s.af
  • Finck, Nathalia Silveira; s.af
  • Garcia, Isis Morosini; s.af
  • Delai, Paola; s.af
Full dent. sci ; 5(17): 157-162, jan. 2014. ilus, tab
Article in Portuguese | LILACS, BBO - Dentistry | ID: lil-706309
Responsible library: BR1264.1
RESUMO
O estudo in vitro avaliou a estabilidade dimensional de três marcas de hidrocolóides irreversíveis submetidos a três diferentes tempos de vazamento do molde. Para isso, foram utilizadas três marcas comerciais de alginato Jeltrate©/Dentsply, Orthoprint©/Dentsply e Ezact©/Vigodent. Um modelo padrão em acrílico foi confeccionado, onde foi simulado a presen‡a dos elementos dentários 17 (pilar A), 14 (pilar B), 24 (pilar C) e 27 (pilar D). Foram realizadas 36 moldagens, sendo 12 moldes de cada marca comercial, subdivididos em três grupos 4 moldes tiveram o gesso vertido imediatamente após a moldagem; 4 moldes foram armazenados em umidificador e tiveram o gesso vertido 5 minutos após a moldagem e 4 moldes foram também armazenado em umidificador, porém teve o gesso vertido 10 minutos após a moldagem. Em seguida, os modelos tiveram a distância entre os pontos mensuradas (medidas AB, BC e CD) e esses valores foram submetidos … análise estatística por meio da tabela ANOVA para cada medida (AB, BC e CD) e foi comparado se houve diferença entre os três grupos. Os modelos de gesso obtidos não apresentaram alteração dimensional significativa nos tempos de armazenamento utilizados. Portanto, os moldes realizados com as três marcas de hidrocolóides irreversíveis podem ser vertidos tanto após a moldagem quanto em até dez minutos passados da tomada da impressão, sem que isso cause alterações dimensionais significantes nos modelos de gesso
ABSTRACT
The in vitro study evaluated the dimensional stability of three brands of irreversible hydrocolloid submitted to three different casting mold times. For this, we used three alginate trademarks Jeltrate©/Dentsply, Orthoprint©/Dentsply and Ezact©/Vigodent. A standard acrylic model was made simulating the presence of teeth 17 (pillar A), 14 (pillar B), 24 (pillar C), and 27 (pillar D). Thirty-six impressions were made, 12 of each brand divided into three groups 4 impressions were poured immediately after molding; 4 impressions were stored at humidifier and poured into the plaster 5 minutes after casting molds, and 4 were also stored in a humidifier but poured into the plaster 10 minutes after the impression. The distances between points AB, BC and CD were measured and these values were statistically analyzed using ANOVA, and then compared to verify if there was any difference between the three groups. No significant dimensional alterations were observed on the obtained plaster models. Therefore molds prepared with all the three brands of irreversible hydrocolloid may be poured after the impression for up to ten minutes after printing without significant dimensional changes in the plaster models
Subject(s)

Search on Google
Collection: International databases Database: BBO - Dentistry / LILACS Main subject: Colloids / Dental Impression Materials / Dental Materials / Alginates Language: Portuguese Journal: Full dent. sci Journal subject: Dentistry Year: 2014 Document type: Article
Search on Google
Collection: International databases Database: BBO - Dentistry / LILACS Main subject: Colloids / Dental Impression Materials / Dental Materials / Alginates Language: Portuguese Journal: Full dent. sci Journal subject: Dentistry Year: 2014 Document type: Article
...