Importance of air bubbles in the core of coated pellets: Synchrotron X-ray microtomography allows for new insights.
Fahier, J; Muschert, S; Fayard, B; Velghe, C; Byrne, G; Doucet, J; Siepmann, F; Siepmann, J.
Affiliation
  • Fahier J; Univ. Lille, Inserm, CHU Lille, U1008 - Controlled Drug Delivery Systems and Biomaterials, 59000 Lille, France.
  • Muschert S; Univ. Lille, Inserm, CHU Lille, U1008 - Controlled Drug Delivery Systems and Biomaterials, 59000 Lille, France.
  • Fayard B; Novitom, 1 Place Firmin Gautier, 38000 Grenoble, France.
  • Velghe C; Univ. Lille, Inserm, CHU Lille, U1008 - Controlled Drug Delivery Systems and Biomaterials, 59000 Lille, France.
  • Byrne G; Early Development Center, Merck Sharp & Dohme, Hertford Road, Hoddesdon EN11 9BU, UK.
  • Doucet J; Novitom, 1 Place Firmin Gautier, 38000 Grenoble, France.
  • Siepmann F; Univ. Lille, Inserm, CHU Lille, U1008 - Controlled Drug Delivery Systems and Biomaterials, 59000 Lille, France.
  • Siepmann J; Univ. Lille, Inserm, CHU Lille, U1008 - Controlled Drug Delivery Systems and Biomaterials, 59000 Lille, France. Electronic address: juergen.siepmann@univ-lille2.fr.
J Control Release ; 237: 125-37, 2016 09 10.
Article in En | MEDLINE | ID: mdl-27374626
ABSTRACT
High-resolution X-ray microtomography was used to get deeper insight into the underlying mass transport mechanisms controlling drug release from coated pellets. Sugar starter cores were layered with propranolol HCl and subsequently coated with Kollicoat SR, plasticized with 10% TEC. Importantly, synchrotron X-ray computed microtomography (SR-µCT) allowed direct, non-invasive monitoring of crack formation in the film coatings upon exposure to the release medium. Propranolol HCl, as well as very small sugar particles from the pellets' core, were expulsed through these cracks into the surrounding bulk fluid. Interestingly, SR-µCT also revealed the existence of numerous tiny, air-filled pores (varying in size and shape) in the pellet cores before exposure to the release medium. Upon water penetration into the system, the contents of the pellet cores became semi-solid/liquid. Consequently, the air-pockets became mobile and fused together. They steadily increased in size (and decreased in number). Importantly, "big" air bubbles were often located in close vicinity of a crack within the film coating. Thus, they play a potentially crucial role for the control of drug release from coated pellets.