Note: Laser-cut molybdenum grids for a retarding field energy analyzer.
Landheer, K; Kobelev, A A; Smirnov, A S; Bosman, J; Deelen, S; Rossewij, M; de Waal, A C; Poulios, I; Benschop, A F; Schropp, R E I; Rath, J K.
Affiliation
  • Landheer K; Utrecht University, Debye Institute for Nanomaterials Science Physics of Devices, High Tech Campus 21, 5656 AE Eindhoven, The Netherlands.
  • Kobelev AA; Peter the Great St. Petersburg Polytechnic University, Department of Plasma Physics, Polytechnicheskaya 29, 195251, St. Petersburg, Russia.
  • Smirnov AS; Peter the Great St. Petersburg Polytechnic University, Department of Plasma Physics, Polytechnicheskaya 29, 195251, St. Petersburg, Russia.
  • Bosman J; ECN - Solliance, High Tech Campus 21, 5656 AE Eindhoven, The Netherlands.
  • Deelen S; Utrecht University, Scientific Instrumentation, Sorbonnelaan 4, 3584 CA Utrecht, The Netherlands.
  • Rossewij M; Utrecht University, Scientific Instrumentation, Sorbonnelaan 4, 3584 CA Utrecht, The Netherlands.
  • de Waal AC; Utrecht University, Debye Institute for Nanomaterials Science Physics of Devices, High Tech Campus 21, 5656 AE Eindhoven, The Netherlands.
  • Poulios I; Utrecht University, Debye Institute for Nanomaterials Science Physics of Devices, High Tech Campus 21, 5656 AE Eindhoven, The Netherlands.
  • Benschop AF; VDL ETG Eindhoven b.v., Achtseweg Noord 5, 5651 GG Eindhoven, The Netherlands.
  • Schropp REI; Utrecht University, Debye Institute for Nanomaterials Science Physics of Devices, High Tech Campus 21, 5656 AE Eindhoven, The Netherlands.
  • Rath JK; Utrecht University, Debye Institute for Nanomaterials Science Physics of Devices, High Tech Campus 21, 5656 AE Eindhoven, The Netherlands.
Rev Sci Instrum ; 88(6): 066108, 2017 Jun.
Article in En | MEDLINE | ID: mdl-28667947
A retarding field energy analyzer (RFEA) with grids created by laser-cutting a honeycomb mesh in a 50 µm thick molybdenum foil is presented. The flat grids span an area of 1 cm2 and have high transmission (20 µm wide walls between 150 µm wide meshes). The molybdenum grids were tested in a 3-grid RFEA configuration with an analyzer depth of 0.87 mm.