Your browser doesn't support javascript.
loading
ZnO Nano-swirlings for Azo Dye AR183 photocatalytic degradation and antimycotic activity.
Umar, Khalid; Mfarrej, Manar Fawzi Bani; Rahman, Qazi Inamur; Zuhaib, Mohammad; Khan, Amir; Zia, Qamar; Banawas, Saeed; Nadeem, Hera; Khan, Mohd Farhan; Ahmad, Faheem.
Affiliation
  • Umar K; School of Chemical Sciences, Universiti Sains Malaysia, 11800, Gelugor, Pulau Pinang, Malaysia.
  • Mfarrej MFB; Department of Life and Environmental Sciences, College of Natural and Health Sciences, Zayed University, 144534, Abu Dhabi, United Arab Emirates.
  • Rahman QI; Department of Chemistry, Integral University, Lucknow, 226026, India.
  • Zuhaib M; Department of Agriculture, School of Sciences, Noida International University, Gautambuddha Nagar, 203201, India.
  • Khan A; Department of Botany, Aligarh Muslim University, Aligarh, 202002, India.
  • Zia Q; Health and Basic Science Research Centre, Majmaah University, Al-Majmaah, 11952, Saudi Arabia.
  • Banawas S; Department of Medical Laboratory Sciences, College of Applied Medical Sciences, Majmaah University, Al-Majmaah, 11952, Saudi Arabia.
  • Nadeem H; Health and Basic Science Research Centre, Majmaah University, Al-Majmaah, 11952, Saudi Arabia.
  • Khan MF; Department of Medical Laboratory Sciences, College of Applied Medical Sciences, Majmaah University, Al-Majmaah, 11952, Saudi Arabia.
  • Ahmad F; Department of Biomedical Sciences, Oregon State University, Corvallis, OR, 97331, USA.
Sci Rep ; 12(1): 14023, 2022 08 18.
Article in En | MEDLINE | ID: mdl-35982131
ABSTRACT
The sol-gel technique was used to fabricate ZnO Nano-swirlings (ZNsw) at a predetermined agitation rate (of >> 1900 rpm), with around 21.94 gm of zinc acetate dihydrate and 0.2 g cetyltrimethylammoniumbromide (CTAB) and a cationic surfactant (drop-wise). The impact of the predetermined agitation condition on the molecular size and morphology of ZNsw is examined, and the outcomes are dissected by useful characterization tools and techniques viz. XRD, SEM embedded with EDS, TEM, FT-IR and UV-visible. The SEM and TEM results suggest that the product formed into a big cluster of adequate ZNsw, containing a significant quantity of folded long thread-lengths. Each group indicated a fair amount of the volume of these lengths. The photocatalytic process of ZNsw was carried out as a result of the irradiation time due to the deterioration of Azo Dye AR183, resulting in approximately 79 percent dye discoloration following an 80-min UV light irradiation in the presence of ZNsw. Additionally, the synthesized ZNsw was tested for antagonistic activity, and the growth hindrance of two plant pathogenic fungal strains found. Per cent inhibition in growth of Rhizoctonia solani and Alternaria alternata were observed in response to ZNsw.