Your browser doesn't support javascript.
loading
Effect of Chemical Treatment of Sugar Palm Fibre on Rheological and Thermal Properties of the PLA Composites Filament for FDM 3D Printing.
Nasir, Mohd Hakim Mohd; Taha, Mastura Mohammad; Razali, Nadlene; Ilyas, Rushdan Ahmad; Knight, Victor Feizal; Norrrahim, Mohd Nor Faiz.
Affiliation
  • Nasir MHM; Faculty of Mechanical Engineering, Universiti Teknikal Malaysia Melaka, Hang Tuah Jaya, Durian Tunggal 76100, Malaysia.
  • Taha MM; Faculty of Mechanical and Manufacturing Engineering Technology, Universiti Teknikal Malaysia Melaka, Hang Tuah Jaya, Durian Tunggal 76100, Malaysia.
  • Razali N; Faculty of Mechanical Engineering, Universiti Teknikal Malaysia Melaka, Hang Tuah Jaya, Durian Tunggal 76100, Malaysia.
  • Ilyas RA; Faculty of Chemical and Energy Engineering, Universiti Teknologi Malaysia (UTM), Johor Bahru 81310, Malaysia.
  • Knight VF; Centre for Advanced Composite Materials, Universiti Teknologi Malaysia (UTM), Johor Bahru 81310, Malaysia.
  • Norrrahim MNF; Institute of Tropical Forest and Forest Products (INTROP), Universiti Putra Malaysia, Serdang 43400, Malaysia.
Materials (Basel) ; 15(22)2022 Nov 15.
Article in En | MEDLINE | ID: mdl-36431566
The thermal and rheological properties of bio-composite filament materials are crucial characteristics in the development of a bio-composite Fused Deposition Modeling (FDM) filament since the printing mechanism of FDM strongly depends on the heating and extrusion process. The effect of chemical treatment on the thermal and rheological properties was investigated to develop composite filaments for FDM using natural fibres such as sugar palm fibre (SPF). SPF underwent alkaline and silane treatment processes before being reinforced with PLA for improving adhesion and removing impurities. Thermogravimetric Analysis (TGA), Differential Scanning Calorimetric (DSC), and Melt Flow Index (MFI) analyses were conducted to identify the differences in thermal properties. Meanwhile, a rheological test was conducted to investigate the shear stress and its viscosity. The TGA test shows that the SPF/PLA composite treated with NaOH and silane showed good thermal stability at 789.5 °C with 0.4% final residue. The DSC results indicate that the melting temperature of all samples is slightly the same at 155 °C (in the range of 1 °C), showing that the treatment does not interfere with the melting temperature of the SPF/PLA composite. Thus, the untreated SPF/PLA composite showed the highest degradation temperature, which was 383.2 °C. The SPF/PLA composite treated with NaOH and silane demonstrated the highest melt flow index of 17.6 g/min. In conclusion, these findings offer a reference point for determining the filament extrusion and printability of SPF/PLA composite filaments.