Improved PVC/ZnO Nanocomposite Insulation for High Voltage and High Temperature Applications.
Khattak, Abraiz; Alahmadi, Ahmad Aziz; Ishida, Hatsuo; Ullah, Nasim.
Affiliation
  • Faiza; School of Natural Sciences, National University of Sciences and Technology (NUST), Sector H-12, Islamabad, 44000, Pakistan.
  • Khattak A; Department of Electrical Power Engineering, National University of Science and Technology, USPCAS-E, Sector H-12, Islamabad, 44000, Pakistan.
  • Alahmadi AA; Department of Macromolecular Science and Engineering, Case Western Reserve University, 10900 Euclid Avenue, Cleveland, OH, 44106-7202, USA.
  • Ishida H; Department of Electrical Power Engineering, National University of Science and Technology, USPCAS-E, Sector H-12, Islamabad, 44000, Pakistan. abraiz@uspcase.nust.edu.pk.
  • Ullah N; Department of Electrical Engineering, College of Engineering, Taif University, PO Box 11099, Taif, 21944, Saudi Arabia.
Sci Rep ; 13(1): 7235, 2023 May 04.
Article in En | MEDLINE | ID: mdl-37142579
Nanosized inorganic oxides have the trends to improve many characteristics of solid polymer insulation. In this work, the characteristics of improved poly (vinyl chloride) (PVC)/ZnO are evaluated using 0, 2, 4 and 6 phr of ZnO nanoparticles dispersed in polymer matrix using internal mixer and finally compressed into circular disk with 80 mm diameter using compression molding technique. Dispersion properties are studied by scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FTIR), X-ray diffractometry (XRD), and optical microscopy (OM). The effect of filler on the electrical, optical, thermal, and dielectric properties of the PVC are also analyzed. Hydrophobicity of nano-composites is evaluated by measuring contact angle and recording hydrophobicity class using Swedish transmission research institute (STRI) classification method. Hydrophobic behavior decreases with the increase in filler content; contact angle increases up to 86°, and STRI class of HC3 for PZ4 is observed. Thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC) are employed to evaluate the thermal properties of the samples. Also, continuous decrease of optical band gap energy from 4.04 eV for PZ0 to 2.57 eV for PZ6 is observed. In the meantime, an enhancement in the melting temperature, Tm, is observed from 172 to 215 °C. To check the stability of materials against hydrothermal stresses, all the fabricated materials are then subjected to a hydrothermal aging process for 1000 h and their structural stability is analyzed using optical microscopy and FTIR analyses.