Your browser doesn't support javascript.
loading
Ferroelectricity in Ultrathin HfO2-Based Films by Nanosecond Laser Annealing.
Athle, Robin; Hill, Megan O; Irish, Austin; Chen, Huaiyu; Timm, Rainer; Kristensson, Elias; Wallentin, Jesper; Borg, Mattias.
Affiliation
  • Athle R; Electrical and Information Technology, Lund University, Box 118, Lund 22 100, Sweden.
  • Hill MO; NanoLund, Lund University, Box 118, Lund 22 100, Sweden.
  • Irish A; NanoLund, Lund University, Box 118, Lund 22 100, Sweden.
  • Chen H; Division of Synchrotron Radiation Research, Lund University, Box 118, Lund 22 100, Sweden.
  • Timm R; MAX IV Laboratory, Lund University, Box 118, Lund 22 100, Sweden.
  • Kristensson E; NanoLund, Lund University, Box 118, Lund 22 100, Sweden.
  • Wallentin J; Division of Synchrotron Radiation Research, Lund University, Box 118, Lund 22 100, Sweden.
  • Borg M; NanoLund, Lund University, Box 118, Lund 22 100, Sweden.
Article in En | MEDLINE | ID: mdl-39359120
ABSTRACT
Nonvolatile memory devices based on ferroelectric HfxZr1-xO2 (HZO) show great promise for back-end integrable storage and for neuromorphic accelerators, but their adoption is held back by the inability to scale down the HZO thickness without violating the strict thermal restrictions of the Si CMOS back end of line. In this work, we overcome this challenge and demonstrate the use of nanosecond pulsed laser annealing (NLA) to locally crystallize areas of an ultrathin (3.6 nm) HZO film into the ferroelectric orthorhombic phase. Meanwhile, the heat induced by the pulsed laser is confined to the layers above the Si, allowing for back-end compatible integration. We use a combination of electrical characterization, nanofocused scanning X-ray diffraction (nano-XRD), and synchrotron X-ray photoelectron spectroscopy (SXPS) to gain a comprehensive view of the change in material and interface properties by systematically varying both laser energy and the number of laser pulses on the same sample. We find that NLA can provide remanent polarization up to 2Pr= 11.6 µC/cm2 in 3.6 nm HZO, albeit with a significant wake-up effect. The improved TiN/HZO interface observed by XPS explains why device endurance goes beyond 107 cycles, whereas an identical film processed by rapid thermal processing (RTP) breaks already after 106 cycles. All in all, NLA provides a promising approach to scale down the ferroelectric oxide thickness for emerging HZO ferroelectric devices, which is key for their integration in scaled process nodes.
Key words

Full text: 1 Collection: 01-internacional Database: MEDLINE Language: En Journal: ACS Appl Mater Interfaces Journal subject: BIOTECNOLOGIA / ENGENHARIA BIOMEDICA Year: 2024 Document type: Article Affiliation country: Sweden Country of publication: United States