Elucidating failure mechanisms in human femurs during a fall to the side using bilateral digital image correlation.
Grassi, Lorenzo; Kok, Joeri; Gustafsson, Anna; Zheng, Yi; Väänänen, Sami P; Jurvelin, Jukka S; Isaksson, Hanna.
Afiliación
  • Grassi L; Department of Biomedical Engineering, Lund University, Sweden. Electronic address: lorenzo.grassi@bme.lth.se.
  • Kok J; Department of Biomedical Engineering, Lund University, Sweden.
  • Gustafsson A; Department of Biomedical Engineering, Lund University, Sweden.
  • Zheng Y; Department of Physics, Technical University of Denmark, Denmark.
  • Väänänen SP; Department of Applied Physics, University of Eastern Finland, Finland; Department of Radiology, Diagnostic Imaging Center, Kuopio University Hospital, Finland.
  • Jurvelin JS; Department of Applied Physics, University of Eastern Finland, Finland.
  • Isaksson H; Department of Biomedical Engineering, Lund University, Sweden.
J Biomech ; 106: 109826, 2020 06 09.
Article en En | MEDLINE | ID: mdl-32517988
ABSTRACT
An improved understanding of the mechanical properties of human femurs is a milestone towards a more accurate assessment of fracture risk. Digital image correlation (DIC) has recently been adopted to provide full-field strain measurements during mechanical testing of femurs. However, it has typically been used to measure strains on the anterior side of the femur, whereas in both single-leg-stance and sideways fall loading conditions, the highest deformations result on the medial and lateral sides of the femoral neck. The goal of this study was to measure full-field deformations simultaneously on the medial and lateral side of the femoral neck in a configuration resembling a fall to the side. Twelve female cadaver femurs were prepared for DIC measurements and tested in sideways fall at 5 mm/s displacement rate. Two pairs of cameras recorded the medial and lateral side of the femoral neck, and deformations were calculated using DIC. The samples exhibited a two-stage failure first, a compressive collapse on the superolateral side of the femoral neck in conjunction with peak force, followed by complete femoral neck fracture at the force drop following the post-elastic phase. DIC measurements corroborated this observation by reporting no tensile strains above yield limit for the medial side of the neck up to peak force. DIC measurements registered onto the bone micro-architecture showed strain localizations in proximity of cortical pores due to, for instance, blood vessels. This could explain previously reported discrepancies between simulations and experiments in regions rich with large pores, like the superolateral femoral neck.
Asunto(s)
Palabras clave

Texto completo: 1 Colección: 01-internacional Base de datos: MEDLINE Asunto principal: Fracturas del Cuello Femoral / Fémur Límite: Female / Humans Idioma: En Revista: J Biomech Año: 2020 Tipo del documento: Article

Texto completo: 1 Colección: 01-internacional Base de datos: MEDLINE Asunto principal: Fracturas del Cuello Femoral / Fémur Límite: Female / Humans Idioma: En Revista: J Biomech Año: 2020 Tipo del documento: Article