Effect of active application of self-etching ceramic primer on the long-term bond strength of different dental CAD/CAM materials.
J Clin Exp Dent
; 13(11): e1089-e1095, 2021 Nov.
Article
en En
| MEDLINE
| ID: mdl-34824694
ABSTRACT
BACKGROUND:
The objective of this in vitro study was to evaluate the effect of the active application of self-etching ceramic primer (ME&P) on the bond strength of different dental CAD/CAM materials (Lithium Disilicate ceramic (LD), Leucite ceramic (LE), Zirconia reinforced lithium silicate ceramic (ZLS), and Hybrid ceramic (HC)) with thermocycling aging. MATERIAL ANDMETHODS:
The samples were randomly divided into 16 groups (n = 20). Dual resin cement cylinders were made and light cured for 10 s (1.200 mW/cm2) for the shear bond strength test. 3-way ANOVA revealed that the factors were statistically significant (P< 0.05).RESULTS:
The aging process had a negative impact on the bond strength for all groups except for Lithium Disilicate, with active application. ZLS and LE showed promising results with high bond strength values for the ME&P active application; however, after aging the bond strength value was significantly reduced. HC showed reduced bond strength values regardless the ME&P application.CONCLUSIONS:
In order to obtain a durable bond strength, the recommended protocol of 20 s of active application followed by 40 s of sitting time in the self-etching ceramic primer should be followed when using reinforced-glass ceramics as restorative materials. Key wordsDentistry, dental materials, silane, shear strength, computer-aided design.
Texto completo:
1
Colección:
01-internacional
Base de datos:
MEDLINE
Idioma:
En
Revista:
J Clin Exp Dent
Año:
2021
Tipo del documento:
Article
País de afiliación:
Brasil