Evaluation of Various Polishing Systems for Lithium Disilicate Glass-Ceramics.
Lee, Y-J; Huh, Y-H; Ko, K-H; Park, C-J; Cho, L-R.
Afiliación
  • Lee YJ; Department of Prosthodontics and Research Institute of Oral Science, College of Dentistry, Gangneung-Wonju National University.
  • Huh YH; Department of Prosthodontics and Research Institute of Oral Science, College of Dentistry, Gangneung-Wonju National University.
  • Ko KH; Department of Prosthodontics and Research Institute of Oral Science, College of Dentistry, Gangneung-Wonju National University.
  • Park CJ; Department of Prosthodontics and Research Institute of Oral Science, College of Dentistry, Gangneung-Wonju National University.
  • Cho LR; Department of Prosthodontics and Research Institute of Oral Science, College of Dentistry, Gangneung-Wonju National University.
Eur J Prosthodont Restor Dent ; 30(3): 188-199, 2022 Aug 30.
Article en En | MEDLINE | ID: mdl-34862863
ABSTRACT

OBJECTIVE:

The aim of this study was to investigate the surface roughness of lithium disilicates (LS2s) polished using various polishing systems. MATERIALS AND

METHODS:

Two types of LS2 (A, Amber Mill and E, IPS e.max CAD) were polished using LS2-specific polishing systems (L-Edenta, L-Jota), a zirconia-specific polishing system (Z-Jota), and a conventional ceramic polishing system (P-Shofu) (n = 8 per group). The compositions of different polishing systems were analyzed using EDS. Surface roughness was measured using confocal laser scanning microscopy and analyzed using EDS and SEM. ANOVA and Tukey's tests were used for the statistical analyses (p = 0.05).

RESULTS:

The polishing systems were mainly composed of C, O, and Si. The L-Jota group exhibited rougher surfaces than the other groups. Amber Mill exhibited higher surface roughness than IPS e.max CAD (p⟨0.001). Among the polishing systems, the L-Jota group presented the highest roughness value (pp⟨0.001). The surface roughness of the AL-Jota group was higher than that of the other groups.

CONCLUSIONS:

A sufficiently smooth surface can be achieved without a LS2-specific polishing system. Further, the same polishing system can have different effects depending on the type of LS2.
Asunto(s)