MgCr2O4-Modified CuO/Cu2O for High-Temperature Thermochemical Energy Storage with High Redox Activity and Sintering Resistance.
Deng, Jiali; Gu, Changdong; Xu, Haoran; Xiao, Gang.
Afiliación
  • Deng J; State Key Laboratory of Clean Energy Utilization, College of Energy Engineering, Zhejiang University, Hangzhou, Zhejiang 310027, China.
  • Gu C; State Key Laboratory of Silicon Materials, College of Materials Science and Engineering, Zhejiang University, Hangzhou, Zhejiang 310027, China.
  • Xu H; State Key Laboratory of Clean Energy Utilization, College of Energy Engineering, Zhejiang University, Hangzhou, Zhejiang 310027, China.
  • Xiao G; State Key Laboratory of Clean Energy Utilization, College of Energy Engineering, Zhejiang University, Hangzhou, Zhejiang 310027, China.
ACS Appl Mater Interfaces ; 14(38): 43151-43162, 2022 Sep 28.
Article en En | MEDLINE | ID: mdl-36121070

Texto completo: 1 Colección: 01-internacional Base de datos: MEDLINE Idioma: En Revista: ACS Appl Mater Interfaces Asunto de la revista: BIOTECNOLOGIA / ENGENHARIA BIOMEDICA Año: 2022 Tipo del documento: Article País de afiliación: China Pais de publicación: Estados Unidos

Texto completo: 1 Colección: 01-internacional Base de datos: MEDLINE Idioma: En Revista: ACS Appl Mater Interfaces Asunto de la revista: BIOTECNOLOGIA / ENGENHARIA BIOMEDICA Año: 2022 Tipo del documento: Article País de afiliación: China Pais de publicación: Estados Unidos