Your browser doesn't support javascript.
loading
Enhancing biomass conversion: Efficient hemicellulose removal and cellulose saccharification in poplar with FeCl3 coupled with acidic electrolyzed water pretreatment.
Chen, Xiaomiao; Liu, Qianjing; Wang, Na; Liu, Caoyunrong; Shi, Jiping; Liu, Li.
Afiliación
  • Chen X; Shanghai Advanced Research Institute, Chinese Academy of Sciences, Shanghai 201210, China; School of Life Science and Technology, ShanghaiTech University, Shanghai 201210, China.
  • Liu Q; Shanghai Advanced Research Institute, Chinese Academy of Sciences, Shanghai 201210, China.
  • Wang N; Shanghai Advanced Research Institute, Chinese Academy of Sciences, Shanghai 201210, China.
  • Liu C; Shanghai Advanced Research Institute, Chinese Academy of Sciences, Shanghai 201210, China; School of Life Science and Technology, ShanghaiTech University, Shanghai 201210, China.
  • Shi J; Shanghai Advanced Research Institute, Chinese Academy of Sciences, Shanghai 201210, China; School of Life Science and Technology, ShanghaiTech University, Shanghai 201210, China. Electronic address: shijp@sari.ac.cn.
  • Liu L; Shanghai Advanced Research Institute, Chinese Academy of Sciences, Shanghai 201210, China; Shanghai Engineering Research Center of Biotransformation of Organic Solid Waste, Shanghai 200241, China. Electronic address: liul@sari.ac.cn.
Int J Biol Macromol ; 253(Pt 8): 127600, 2023 Dec 31.
Article en En | MEDLINE | ID: mdl-37871719
ABSTRACT
Due to the recalcitrant structure of woody biomass such as poplar, the efficient disassembly and separation of hemicellulose component from woody biomass is crucial for green biomass processing and full component utilization. This study presented an environmentally friendly approach to utilize acidic electrolyzed water (AEW) combined with metal salts and investigated its pretreatment effects on hemicellulose removal and cellulose and lignin retention under different conditions. Meanwhile, the structural properties and enzymatic hydrolysis performance of the pretreated residues were also characterized. As a result, under the optimized pretreatment conditions (0.03 mol/L FeCl3 with AEW at 180 °C for 10 min), hemicellulose removal from poplar wood reached 98.64 %, accompanied by xylose recovery rate of 98.46 %, cellulose retention rate of 93.43 % and lignin retention rate of 94.29 %. Enzymatic hydrolysis rate of the pretreated cellulose-enriched substrate reached 97.65 %. Furthermore, comprehensive structural characterizations revealed that FeCl3 coupled with AEW pretreatment resulted in surface damage to the poplar wood, effective removal of the amorphous hemicellulose component, and partial destruction of the cellulose crystallinity. In conclusion, FeCl3 coupled with AEW pretreatment effectively separates hemicellulose, leading to significant alterations in biomass composition and structure, ultimately resulting in improved enzymatic digestion. These results provide theoretical support for targeted dissociation of hemicellulose and full component utilization of woody biomass.
Asunto(s)
Palabras clave

Texto completo: 1 Colección: 01-internacional Base de datos: MEDLINE Asunto principal: Celulosa / Populus Idioma: En Revista: Int J Biol Macromol Año: 2023 Tipo del documento: Article País de afiliación: China

Texto completo: 1 Colección: 01-internacional Base de datos: MEDLINE Asunto principal: Celulosa / Populus Idioma: En Revista: Int J Biol Macromol Año: 2023 Tipo del documento: Article País de afiliación: China