Your browser doesn't support javascript.
loading
Bonding of universal adhesive system to enamel surrounding real-life carious cavities
Pires, Carine Weber; Lenzi, Tathiane Larissa; Department of Restorative DentistrySoares, Fabio Zovico Maxnuck; Rocha, Rachel de Oliveira.
Afiliação
  • Pires, Carine Weber; Centro Universitário da Serra Gaúcha. School of Dentistry. Caxias do Sul. BR
  • Lenzi, Tathiane Larissa; Universidade Federal do Rio Grande do Sul. Department of Surgery and Orthopedics. Porto Alegre. BR
  • Department of Restorative DentistrySoares, Fabio Zovico Maxnuck; Universidade Federal de Santa Maria. School of Dentistry. Department of Restorative DentistrySoares, Fabio Zovico Maxnuck. Santa Maria. BR
  • Rocha, Rachel de Oliveira; Universidade Federal de Santa Maria. Department of Stomatology. Santa Maria. BR
Braz. oral res. (Online) ; 33: e038, 2019. tab, graf
Artigo em Inglês | LILACS | ID: biblio-1001609
Biblioteca responsável: BR1.1
ABSTRACT
Abstract This study aimed to evaluate the bond strength of a universal adhesive system to enamel surrounding real-life carious cavities. Twenty-eight permanent molars (n = 7) with carious lesions in dentin were subjected to selective carious tissue removal to firm dentin and had their crowns sectioned longitudinally. A universal adhesive system (Single Bond Universal [SBU] used in either etch-and-rinse and self-etch strategies) was compared with an etch-and-rinse Adper Single Bond 2 (ASB) and a self-etch Clearfil SE Bond (CSE) adhesive systems (control systems). Adhesives were applied on the enamel, assumed demineralized, surrounding the cavity margins and on sound enamel (control substrate). Composite cylinders were built (0.72 mm2) and microshear bond strength (µSBS) test was performed after 24 h of water storage. The µSBS values (MPa) were analyzed using two-way ANOVA and Tukey's post hoc tests (α = 0.05). Bond strength values obtained in demineralized enamel surrounding carious cavity margins were significantly lower than that obtained in sound enamel (distant from carious cavity margins) (p = 0.035). The bonding strategy of the SBU did not influenced the bond strength values, which were higher than that obtained with ASB. CSE showed similar µSBS values to ASB and SBU in the self-etch mode. In conclusion, the bond strength to enamel assumed demineralized is lower than to sound enamel. The enamel surrounding carious cavities jeopardize the bonding of universal adhesive system. The bond strength of universal adhesive is similar, regardless to bonding strategy.
Assuntos


Texto completo: Disponível Coleções: Bases de dados internacionais Base de dados: LILACS Assunto principal: Colagem Dentária / Bis-Fenol A-Glicidil Metacrilato / Cárie Dentária / Cimentos Dentários / Esmalte Dentário Tipo de estudo: Ensaio clínico controlado / Estudo de avaliação Limite: Humanos Idioma: Inglês Revista: Braz. oral res. (Online) Assunto da revista: Odontologia Ano de publicação: 2019 Tipo de documento: Artigo País de afiliação: Brasil Instituição/País de afiliação: Centro Universitário da Serra Gaúcha/BR / Universidade Federal de Santa Maria/BR / Universidade Federal do Rio Grande do Sul/BR

Texto completo: Disponível Coleções: Bases de dados internacionais Base de dados: LILACS Assunto principal: Colagem Dentária / Bis-Fenol A-Glicidil Metacrilato / Cárie Dentária / Cimentos Dentários / Esmalte Dentário Tipo de estudo: Ensaio clínico controlado / Estudo de avaliação Limite: Humanos Idioma: Inglês Revista: Braz. oral res. (Online) Assunto da revista: Odontologia Ano de publicação: 2019 Tipo de documento: Artigo País de afiliação: Brasil Instituição/País de afiliação: Centro Universitário da Serra Gaúcha/BR / Universidade Federal de Santa Maria/BR / Universidade Federal do Rio Grande do Sul/BR
...