ABSTRACT
Aim:
To evaluate the bond strength (BS) and failure mode of orthodontic tubes treated with different alloy primers at the interface among enamel, resin and orthodontic tubes.Methods:
Orthodontic tubes were bonded to the enamel of 80 bovine incisors with the orthodontic resin (Transbond XT, 3M Unitek). Prior to bonding, the tubes were chemically treated with (n=20) Metal/Zirconia Primer (MZ, Ivoclar), Scothbond Universal (SB, 3M Espe); Orthoprimer (OP, Morelli) or left untreated (Control - C). Specimens were submitted to 5,000 thermal cycles (5 and 55o C) to age the bonded interface. A shear BS test and failure modes were conducted, and the results were analyzed using one-way analysis of variance and Fisher's exact test, respectively.Results:
No differences were observed among groups regardless of the type of alloy primer used (p = 0.254). However, no differences were observed among the failure modes of the groups tested (p=0.694). The adhesive failure mode between the resin and enamel was the most prevalent failure (45%) for groups OP and C, whereas cohesive failure in the orthodontic resin was the most prevalent failure (40%) for groups SB and MZ.Conclusion:
Alloy primers were unable to increase the BS of the orthodontic tubes to enamel
Texto completo:
Disponível
Coleções:
Bases de dados internacionais
Base de dados:
BBO - Odontologia
/
LILACS
Assunto principal:
Ortodontia
/
Teste de Materiais
/
Colagem Dentária
/
Resistência ao Cisalhamento
Limite:
Animais
Idioma:
Inglês
Revista:
Braz. j. oral sci
Assunto da revista:
Odontologia
Ano de publicação:
2019
Tipo de documento:
Artigo
País de afiliação:
Brasil
Instituição/País de afiliação:
Institute and Research Center São Leopoldo Mandic/BR
/
University of Campinas/BR