Efeito do processo erosivo causado por diferentes bebidas na resistência a união de diferentes sistemas adesivos em superfície de esmalte: análise in vitro e in situ/ex vivo / Effect of erosive process caused by different beverages on bond strength of different bonding systems to enamel: in vitro and in situ/ex vivo analyses
Bauru; s.n; 2011. 119 p. ilus, tab, graf.
Tese em Português | LILACS, BBO - Odontologia | ID: lil-668585
Biblioteca responsável: BR28.1
RESUMO
A erosão dentária consiste em uma das causas de desgaste dentário que acomete inicialmente o esmalte, por meio de um amolecimento da superfície, podendo comprometer também a dentina. A compreensão do mecanismo erosivo permite determinar estratégias para sua prevenção, controle e tratamento. Em função do comprometimento do esmalte, esse substrato requer, em alguns casos, o tratamento por meio de restauração adesiva. Este trabalho consta de três fases e teve por objetivo analisar a união de diferentes sistemas adesivos a superfícies de esmalte, após ciclagem erosiva in vitro e in situ/ex vivo. Inicialmente, um estudo in vitro foi realizado envolvendo desafios por 3x/1minutos/1dia por 3 bebidas erosivas à base de cola (Coca-Cola Regular, Coca Light e Coca Zero) associados ou não à escovação. Fragmentos de esmalte bovino foram adequadamente obtidos, polidos e selecionados através de teste de microdureza. Após os desafios, foram restaurados com o sistema convencional de dois passos Adper Single Bond 2 e preparados para testes quantitativos de desgaste, microdureza, e de resistência adesiva e qualitativa por microscopia de varredura confocal a laser. Uma vez que a Coca-Cola Regular foi o agente mais erosivo, as demais fases foram realizadas unicamente com sua utilização. Assim, as hipóteses nulas testadas nas duas fases seguintes foram 1- Não há diferença de adesão ao esmalte normal ou erodido/abrasionado; 2- Não há diferença de adesão ao esmalte erodido/abrasionado de acordo com o sistema adesivo utilizado. Para os testes in vitro, os mesmos passos foram seguidos, entretanto, com desafios erosivos de 3x/1min de imersão por 1 ou 5 dias, associados ou não à escovação. No teste in situ/ex vivo, 8 fragmentos de esmalte foram preparados para cada dispositivo intrabucal. A cada 24 horas, os voluntários efetuaram 3 ciclos extrabucais de 3x/5min em Coca-Cola em metade dos blocos. Metade dos blocos não erodidos e erodidos foram seqüencialmente escovados por ...
ABSTRACT
Tooth erosion is considered a cause of dental wear with initial softening of enamel, which can also compromise dentin. The comprehension of erosive mechanism aids to determine its strategies of prevention, control and treatment. According to enamel compromising, it requires in some cases, an adhesive restoration approach. This study consisted of three phases and aimed to analyze adhesion of different bonding systems to enamel surface after in vitro and in situ/ex vivo erosive cycles. First, an in vitro experiment was performed involving 3 colabased beverages (Regular Coke, Light Coke and Zero Coke) challenged for 3x/1min for a day associated or not to toothbrushing. Enamel specimens were adequately prepared, polished and selected by microhardness. After challenges, they were restored by a two-step etch-and-rinse system (Adper Single Bond 2), which were prepared to quantitative tests of wear, microhardness and bonding and also qualitative analysis using confocal laser scanning microscopy. As Regular Coke was the most erosive agent, the following phases only used this beverage. Thus the null hypotheses were 1- There is no difference on bonding to normal or eroded/abraded enamel surface; 2- There is no difference on bonding to eroded/abraded enamel according to dentin bonding system. For in vitro tests, same previous steps were performed however with erosive challenges for 3x/1min for 1 and 5 days, immediately associated or not to 1-minute toothbrushing. In in situ/ex vivo test, 8 specimens were prepared for each intraoral palatal device. Volunteers performed erosive challenge extraorally on half of the specimes in Regular Coke for 3x/5min for 5 days. Half of the not eroded and eroded specimens were subsequently abraded for 1 minute. After the end of 5 days, the devices were collected and the specimens were identified. After in vitro or in situ/ex vivo, enamel surfaces were restored with different dentin bonding...
Assuntos

Texto completo: Disponível Coleções: Bases de dados internacionais Base de dados: BBO - Odontologia / LILACS Assunto principal: Erosão Dentária / Bebidas Gaseificadas / Adesivos Dentinários / Esmalte Dentário / Dentina Tipo de estudo: Estudo prognóstico / Pesquisa qualitativa Limite: Animais Idioma: Português Ano de publicação: 2011 Tipo de documento: Tese
Texto completo: Disponível Coleções: Bases de dados internacionais Base de dados: BBO - Odontologia / LILACS Assunto principal: Erosão Dentária / Bebidas Gaseificadas / Adesivos Dentinários / Esmalte Dentário / Dentina Tipo de estudo: Estudo prognóstico / Pesquisa qualitativa Limite: Animais Idioma: Português Ano de publicação: 2011 Tipo de documento: Tese
...