1.
Mar Pollut Bull ; 198: 115830, 2024 Jan.
Artigo em Inglês | MEDLINE | ID: mdl-37995594

RESUMO

The present work was conducted to characterize the mangrove sediments along the Egyptian Red Sea in terms of elemental composition and to assess the extent of pollution and its sources. A total of 26 samples of mangrove sediments were collected from three different areas: Sharm El Madfea, Sowmaa Mangrove and Abu Fasi. The samples were analyzed using the inductively coupled plasma - mass spectrometry ICP-MS and atomic-emission spectrometry ICP-AES. Mass fractions of a total of 58 major and trace elements were determined in the mangrove samples. Univariate and multivariate statistical analyses were performed to determine the origin of trace and major elements in the mangrove sediments. The normalized values show that the elements above the background can be indicated in descending order as follows: P > Cd > Sr > Ca > U > Se > As > Sn > Cu > Sb > Pb > Mo > Ag. Several pollution indices were also calculated. Principal component analysis revealed three clusters of the studied sediment samples. The analysis of the ratio indicators shows that the origin of the sediments mostly falls near continental island arcs (CIA). The pollution indices show remarkable pollution levels and enriched elements. The data obtained can serve as baseline data for the sediments of the mangrove environment and can be used to study possible changes in the future.


Assuntos
Metais Pesados , Poluentes Químicos da Água , Oceano Índico , Egito , Sedimentos Geológicos/química , Poluentes Químicos da Água/análise , Monitoramento Ambiental , Metais/análise , Metais Pesados/análise
2.
Materials (Basel) ; 14(22)2021 Nov 10.
Artigo em Inglês | MEDLINE | ID: mdl-34832170

RESUMO

Melt quenching technique is used for preparing glasses with chemical formula (70P2O5)-(16 - x)CdO-(14ZnO)-(xEr2O3), (x = 1-6 mol%). These glasses were named Er1, Er2, Er3, Er4, Er5, and Er6, respectively. Photon buildup factors, fast neutron absorption, and electron stopping of the prepared glasses were examined. Glasses' density was varied from 3.390 ± 0.003 for the Er1 glass sample to 3.412 ± 0.003 for the Er6 glass sample. The Buildup factor (BUF) spectra have relatively higher values in the Compton Scattering (CS) dominated areas compared to both Photoelectric effect (PE), and Pair Production (PP) dominated energy regions. The highest BUF appeared at the Er atom K-absorption edge, whose intensity increases as the molar concentration of Er2O3 in the glasses increases. The photon absorption efficiency (PAE) of the glasses increases according to the trend (PAE)Er1 < (PAE)Er2 < (PAE)Er3 < (PAE)Er4 < (PAE)Er5 < (PAE)Er6. Fast neutron removal cross-section, FNRC (ΣR) values of the glasses obtained via calculation varied from 0.1045-0.1039 cm-1 for Er1-Er6. Furthermore, the continuous slowing down approximation mode (CSDA) range enhances the kinetic energy of electrons for all glasses. Generally, results revealed that the investigated glasses could be applied for radiation shielding and dosimetric media.

3.
Appl Spectrosc ; 68(2): 192-7, 2014.
Artigo em Inglês | MEDLINE | ID: mdl-24480275

RESUMO

An accurate technique has been developed to calculate the equivalent width of absorption lines. The calculations have been carried out for the pure Doppler and pure Lorentz limiting forms of the equivalent width. A novel expression for the equivalent width for Lorentz profile is given from direct integration of the line profile. The more general case of a Voigt profile leads to an analytical formula that permits a rapid estimate of the equivalent width for a wide range of maximum optical depths. The reliability of the approach is verified using a numerical application calculating the equivalent width for nickel resonance lines at 232.0 and 352.3 nm from atomic absorption (AA) measurements. The dependence of equivalent width on the number density of absorbing atoms is also provided. The results obtained for the equivalent width for the Voigt profile were compared with the data in the available literature obtained by different approaches.