Your browser doesn't support javascript.
loading
Low-Temperature and Fast-Charge Sodium Metal Batteries.
Yu, Dandan; Wang, Zhenya; Yang, Jiacheng; Wang, Yingyu; Li, Yuting; Zhu, Qiaonan; Tu, Xinman; Chen, Dezhi; Liang, Junfei; Khalilov, Umedjon; Wang, Hua.
Afiliação
  • Yu D; Key Laboratory of Jiangxi Province for Persistent Pollutants Control and Resources Recycle, School of Environmental and Chemical Engineering, Nanchang Hangkong University, Nanchang, 330063, China.
  • Wang Z; College of Materials and Chemistry, China Jiliang University, Hangzhou, 310018, China.
  • Yang J; School of Chemistry, Beijing Advanced Innovation Center for Biomedical Engineering, Beihang University, Beijing, 100191, China.
  • Wang Y; School of Chemistry, Beijing Advanced Innovation Center for Biomedical Engineering, Beihang University, Beijing, 100191, China.
  • Li Y; School of Chemistry, Beijing Advanced Innovation Center for Biomedical Engineering, Beihang University, Beijing, 100191, China.
  • Zhu Q; School of Chemistry, Beijing Advanced Innovation Center for Biomedical Engineering, Beihang University, Beijing, 100191, China.
  • Tu X; School of Chemistry, Beijing Advanced Innovation Center for Biomedical Engineering, Beihang University, Beijing, 100191, China.
  • Chen D; Key Laboratory of Jiangxi Province for Persistent Pollutants Control and Resources Recycle, School of Environmental and Chemical Engineering, Nanchang Hangkong University, Nanchang, 330063, China.
  • Liang J; Key Laboratory of Jiangxi Province for Persistent Pollutants Control and Resources Recycle, School of Environmental and Chemical Engineering, Nanchang Hangkong University, Nanchang, 330063, China.
  • Khalilov U; School of Energy and Power Engineering, North University of China, Taiyuan, 030051, China.
  • Wang H; Department of Chemistry, University of Antwerp, Universiteitsplein 1, Antwerp, 2610, Belgium.
Small ; 20(30): e2311810, 2024 Jul.
Article em En | MEDLINE | ID: mdl-38385819
ABSTRACT
Low-temperature operation of sodium metal batteries (SMBs) at the high rate faces challenges of unstable solid electrolyte interphase (SEI), Na dendrite growth, and sluggish Na+ transfer kinetics, causing a largely capacity curtailment. Herein, low-temperature and fast-charge SMBs are successfully constructed by synergetic design of the electrolyte and electrode. The optimized weak-solvation dual-salt electrolyte enables high Na plating/stripping reversibility and the formation of NaF-rich SEI layer to stabilize sodium metal. Moreover, an integrated copper sulfide electrode is in situ fabricated by directly chemical sulfuration of copper current collector with micro-sized sulfur particles, which significantly improves the electronic conductivity and Na+ diffusion, knocking down the kinetic barriers. Consequently, this SMB achieves the reversible capacity of 202.8 mAh g-1 at -20 °C and 1 C (1 C = 558 mA g-1). Even at -40 °C, a high capacity of 230.0 mAh g-1 can still be delivered at 0.2 C. This study is encouraging for further exploration of cryogenic alkali metal batteries, and enriches the electrode material for low-temperature energy storage.