Process and mechanism of preparing metallized blast furnace burden from metallurgical dust and sludge.
Gao, Xing; Chai, Yifan; Wang, Yici; Luo, Guoping; An, Shengli; Peng, Jun.
Afiliação
  • Gao X; School of Metallurgical Future Technology, Inner Mongolia University of Science and Technology, Baotou, 014000, China.
  • Chai Y; Key Laboratory of Green Extraction & Efficient Utilization of Light Rare-Earth Resources (Inner Mongolia University of Science and Technology), Ministry of Education, Baotou, 014010, China.
  • Wang Y; School of Metallurgical Future Technology, Inner Mongolia University of Science and Technology, Baotou, 014000, China. chaiyifan@live.cn.
  • Luo G; Key Laboratory of Green Extraction & Efficient Utilization of Light Rare-Earth Resources (Inner Mongolia University of Science and Technology), Ministry of Education, Baotou, 014010, China. chaiyifan@live.cn.
  • An S; School of Metallurgical Future Technology, Inner Mongolia University of Science and Technology, Baotou, 014000, China.
  • Peng J; School of Metallurgical Future Technology, Inner Mongolia University of Science and Technology, Baotou, 014000, China.
Sci Rep ; 14(1): 9760, 2024 Apr 29.
Article em En | MEDLINE | ID: mdl-38684847
ABSTRACT
Metallurgical dust and sludge are solid waste resources with recycling value. In recent years, rotary hearth furnace has become the most important means to treat metallurgical dust and sludge because of its wide range of raw materials and strong treatment capacity. In this study blast furnace ash and converter sludge were selected as the research objects, and high-quality metallized pellets were prepared based on the rotary hearth furnace process. The strength changed of pellets, the reduction process of iron oxides and the removal process of zinc during the roasting of pellets in rotary hearth furnace were studied. To explore the reasonable roasting condition for preparing metallized pellets in rotary hearth furnace. The optimum roasting temperature of the pellets was 1250℃ and the roasting time was 25 min. The compressive strength, metallization rate and dezincification rate of metallized pellets reached 1361N, 97.44% and 95.67%, respectively. The efficient resource utilization of various metallurgical dust and sludge is realized.