Sci Rep ; 12(1): 8700, 2022 05 24.
Artículo en Inglés | MEDLINE | ID: mdl-35610349

RESUMEN

Novel metal matrix composites (MMCs) have been fabricated with Ti6Al4V matrix and a biogenic ceramic filler in the form of diatomaceous earth (DE). Mixtures of DE and Ti6Al4V powders were consolidated by the spark plasma sintering (SPS) method. Microstructure of the consolidated samples has been investigated with microscopic techniques and XRD. Thermomechanical characteristics have been obtained using small-sample techniques. The results obtained indicate that the fabricated composites show outstanding mechanical and thermal properties due to synergic effects between the filler and the matrix (beyond the rule of mixtures).


Asunto(s)
Cerámica , Titanio , Cerámica/química , Ensayo de Materiales , Titanio/química
2.
Materials (Basel) ; 15(6)2022 Mar 08.
Artículo en Inglés | MEDLINE | ID: mdl-35329457

RESUMEN

Aluminium (Al) and titanium (Ti) coatings were applied on AZ91E magnesium alloy using a low-pressure warm spray (WS) method. The deposition was completed using three different nitrogen flow rates (NFR) for both coatings. NFR effects on coating microstructure and other physical properties were systematically studied. Microstructural characterization was performed using scanning electron microscopy (SEM), and the porosity was estimated using two methods-image analysis and X-ray microtomography. The coating adhesion strength, wear resistance, and hardness were examined. The protective properties of the coatings were verified via a salt spray test. Decreasing NFR during coating deposition produced more dense and compact coatings. However, these conditions increased the oxidation of the powder. Al coatings showed lower hardness and wear resistance than Ti coatings, although they are more suitable for corrosion protection due to their low porosity and high compactness.

3.
Materials (Basel) ; 15(18)2022 Sep 07.
Artículo en Inglés | MEDLINE | ID: mdl-36143522

RESUMEN

The poly(lactic acid) (PLA) biodegradable polymer, as well as natural, siliceous reinforcement in the form of diatomaceous earth, fit perfectly into the circular economy trend. In this study, various kinds of commercial PLA have been reinforced with diatomaceous earth (DE) to prepare biodegradable composites via the extrusion process. The structure of the manufactured composites as well as adhesion between the matrix and the filler were investigated using scanning electron microscopy (SEM). Differential scanning calorimetry (DSC) analyses were carried out to determine crystallinity of PLA matrix as function of DE additions. Additionally, the effect of the ceramic-based reinforcement on the mechanical properties (Young's modulus, elongation to failure, ultimate tensile strength) of PLA has been investigated. The results are discussed in terms of possible applications of PLA + DE composites.

4.
Materials (Basel) ; 15(24)2022 Dec 16.
Artículo en Inglés | MEDLINE | ID: mdl-36556821

RESUMEN

Additive manufacturing (AM) has seen remarkable development in recent years due to relatively high efficiency of the process. Cold spraying (CS) is a particular method of AM, in which titanium and titanium alloy powders are used. CS is a very competitive technology enabling the deposition of coatings, repairing machine parts, and manufacturing new components. For specific applications, the surface of cold-sprayed materials may require further processing. This paper reports an attempt to employ laser surface treatment (LST) of cold-sprayed coatings on an aluminium alloy substrate. The influence of laser beam interaction time on the coatings' properties was analysed. The microstructure was investigated and observed employing scanning electron microscopy (SEM). To evaluate residual stress after CS and LST, the sin2ψ technique was used. Investigations were also performed on Vickers hardness, contact angle, and surface roughness. Significant changes in the surface morphology of the coatings and elevated residual stress levels dependent on the laser beam interaction time were observed. Increased Vickers hardness was recorded for titanium alloy Ti6Al4V. LST also led to increased surface hydrophilicity of the modified materials Ti and Ti6Al4V.

5.
Materials (Basel) ; 14(21)2021 Nov 01.
Artículo en Inglés | MEDLINE | ID: mdl-34772094

RESUMEN

Designers' efforts to use the lightest possible materials with very good mechanical properties mean that in recent years magnesium alloys have been increasingly used. It is well-known that the use of various plastic working processes allows achieving even better strength properties of the material, often without significant loss of plastic properties in relation to the properties of products obtained in the casting process. The article presents the results of research on microstructural changes and mechanical properties of the alloy AZ91 (MgAl9Zn1) occurring in samples subjected to conventional plastic deformation and the KOBO method. The obtained results were compared to the properties of reference samples, i.e., cast samples. The article presents the advantage of using the low-temperature KOBO method compared to the high-temperature deformation in a conventional manner. Moreover, it has been shown that the use of KOBO extrusion allows the alloy AZ91 (MgAl9Zn1) to obtain superplasticity properties with an elongation of up to 577% compared to the cast reference sample, which is generally classified as difficult for plastic deformation.

6.
Materials (Basel) ; 14(19)2021 Sep 23.
Artículo en Inglés | MEDLINE | ID: mdl-34639890

RESUMEN

In this research, the cold spray process as an additive manufacturing method was applied to deposit thick titanium coatings onto 7075 aluminium alloy. An analysis of changes in the microstructure and mechanical properties of the coatings depending on the standoff distance was carried out to obtain the maximum deposition efficiency. The process parameters were selected in such a way as to ensure the spraying of irregular titanium powder at the highest velocity and temperature and changing the standoff distance from 20 to 100 mm. Experimental studies demonstrated that the standoff distance had a significant effect on the microstructure of the coatings and their adhesion. Moreover, its rise significantly increased the deposition efficiency. The standoff distance also significantly affected the coating microstructure and their adhesion to the substrate, but did not cause any changes in their phase composition. The standoff distance also influenced the coating porosity, which first decreased to a minimum level of 0.2% and then increased significantly to 9.8%. At the same time, the hardness of the coatings increased by 30%. Numerical simulations confirmed the results of the tests.

7.
Acta Bioeng Biomech ; 14(3): 75-8, 2012.
Artículo en Inglés | MEDLINE | ID: mdl-23140104

RESUMEN

The use of adhesive bonding systems and composites in prosthetic dentistry brought improved and more aesthetic prosthetic restorations. The adhesive bonding of porcelain veneers is based on the micromechanical and chemical bond between tooth surface, cement layer and ceramic material. The aim of the study was to measure the thickness of the material layer formed during cementing of a ceramic restoration, and - in the second part of the study - to test tension of these cements. The materials investigated comprised dual-curing materials: Variolink II, KoNroot Cem, KoNroot Cem Viscous and Panavia F 2.0, as well as a light-curing composite: Variolink Veneer. The thickness was measured with the use of ZIP Lite 250 optical gauging apparatus. SEM microscope - Hitachi Tabletop Microscope TM-100 - was used to analyse the characteristics of an adhesive bond and filler particle size of particular materials. Tension tests of the cements under study were carried out on the MTS Q Test 10 static electrodynamic apparatus. The tests showed that KoNroot Cem exhibited the best mechanical properties of bonding to enamel and dentin among the materials tested. Variolink II base light-curing cement formed the thinnest layer. All the materials tested formed the layer not exceeding 1/3 of ceramic restoration thickness.


Asunto(s)
Cerámica/química , Recubrimiento Dental Adhesivo , Materiales Dentales/química , Coronas con Frente Estético , Ensayo de Materiales , Fenómenos Mecánicos , Cementos Dentales , Esmalte Dental/ultraestructura , Dentina/ultraestructura