RESUMO
A carbon-nanotube-enabling scanning probe technique/nanotechnology for manipulating and measuring lithium at the nano/mesoscale is introduced. Scanning Li-nanopipette and probe microscopy (SLi-NPM) is based on a conductive atomic force microscope (AFM) cantilever with an open-ended multi-walled carbon nanotube (MWCNT) affixed to its apex. SLi-NPM operation is demonstrated with a model system consisting of a Li thin film on a Si(111) substrate. By control of bias, separation distance, and contact time, attograms of Li can be controllably pipetted to or from the MWCNT tip. Patterned surface Li features are then directly probed via noncontact AFM measurements with the MWCNT tip. The subsequent decay of Li features is simulated with a mesoscale continuum model, developed here. The Li surface diffusion coefficient for a four (two) Li layer thick film is measured as D=8(±1.2)×10(-15) cm(2) s(-1) (D=1.75(±0.15)×10(-15) cm(2) s(-1)). Dual-Li pipetting/measuring with SLi-NPM enables a broad range of time-dependent Li and nanoelectrode characterization studies of fundamental importance to energy-storage research.
RESUMO
The binding configuration of propylene glycol stereoisomer molecules adsorbed on the Si(001)-2×1 surface was investigated using a combination of scanning tunneling microscopy (STM) and density functional theory calculations. Propylene glycol was found to adsorb dissociatively via two hydroxyl groups exclusively as a bridge between the ends of two adjacent dimers along the dimer row. The chirality was preserved during bonding to Si atoms and was identifiable with STM imaging. The large number of propylene glycol conformers in the gas phase was reduced to a single configuration adsorbed on the surface at low molecular coverage.