1.
Artigo em Inglês | MEDLINE | ID: mdl-33304445

RESUMO

Nanoscale wear affects the performance of atomic force microscopy (AFM)-based measurements for all applications including process control measurements and nanoelectronics characterization. As such, methods to prevent or reduce AFM tip wear is an area of active research. However, most prior work has been on conventional AFMs rather than critical dimension AFM (CD-AFM). Hence, less is known about CD-AFM tip-wear. Given that tip-wear directly affects the accuracy of dimensional measurements, a basic understanding of CD-AFM tip wear is needed. Toward this goal, we evaluated the wear performance of electron beam deposited CD-AFM tips. Using a continuous scanning strategy, we evaluated the overall wear rate and tip lifetime and compared these with those of silicon-based CD-AFM tips. Our data show improved tip lifetime of as much as a factor of five and reduced wear rates of more than 17 times. Such improvements in wear rate means less measurement variability and lower cost.

2.
Artigo em Inglês | MEDLINE | ID: mdl-39483644

RESUMO

Since 2004 standards for calibration of critical dimension atomic force microscope (CD-AFM) tip width have been available both commercially and through national metrology institutes (NMIs) - such as the National Institute of Standards and Technology (NIST) in the United States. There have been inter-laboratory and inter-method comparisons performed on such samples, but less attention has been paid to the long-term stability of standards and monitoring for damage, wear, or contamination. Using three different CD-AFM instruments, we have tested the consistency and long-term stability of two independent reference calibrations for CD-AFM tip width. Both of these tip width calibrations were based on independently implemented transmission electron microscope (TEM) reference measurements. There were circumstances in which damage occurred or samples needed to be cleaned. Nevertheless, our results show agreement within the uncertainties and stability over a period exceeding 10 years.

3.
Artigo em Inglês | MEDLINE | ID: mdl-27087883

RESUMO

Sidewall sensing in critical dimension atomic force microscopes (CD-AFMs) usually involves continuous lateral dithering of the tip or the use of a control algorithm and fast response piezo actuator to position the tip in a manner that resembles touch-triggering of coordinate measuring machine (CMM) probes. All methods of tip position control, however, induce an effective tip width that may deviate from the actual geometrical tip width. Understanding the influence and dependence of the effective tip width on the dither settings and lateral stiffness of the tip can improve the measurement accuracy and uncertainty estimation for CD-AFM measurements. Since CD-AFM typically uses tips that range from 15 nm to 850 nm in geometrical width, the behavior of effective tip width throughout this range should be understood. The National Institute of Standards and Technology (NIST) has been investigating the dependence of effective tip width on the dither settings and lateral stiffness of the tip, as well as the possibility of material effects due to sample composition. For tip widths of 130 nm and lower, which also have lower lateral stiffness, the response of the effective tip width to lateral dither is greater than for larger tips. However, we have concluded that these effects will not generally result in a residual bias, provided that the tip calibration and sample measurement are performed under the same conditions. To validate that our prior conclusions about the dependence of effective tip width on lateral stiffness are valid for large CD-tips, we recently performed experiments using a very large non-CD tip with an etched plateau of approximately 2 µm width. The effective lateral stiffness of these tips is at least 20 times greater than typical CD-AFM tips, and these results supported our prior conclusions about the expected behavior for larger tips. The bottom-line importance of these latest observations is that we can now reasonably conclude that a dither slope of 3 nm/V is the baseline response due to the induced motion of the cantilever base.

4.
J Micro Nanolithogr MEMS MOEMS ; 15(3): 034005, 2016 Jul.
Artigo em Inglês | MEDLINE | ID: mdl-27840664

RESUMO

The decreasing size of semiconductor features and the increasing structural complexity of advanced devices have placed continuously greater demands on manufacturing metrology, arising both from the measurement challenges of smaller feature sizes and the growing requirement to characterize structures in more than just a single critical dimension. For scanning electron microscopy, this has resulted in increasing sophistication of imaging models. For critical dimension atomic force microscopes (CD-AFMs), this has resulted in the need for smaller and more complex tips. Carbon nanotube (CNT) tips have thus been the focus of much interest and effort by a number of researchers. However, there have been significant issues surrounding both the manufacture and use of CNT tips. Specifically, the growth or attachment of CNTs to AFM cantilevers has been a challenge to the fabrication of CNT tips, and the flexibility and resultant bending artifacts have presented challenges to using CNT tips. The Korea Research Institute for Standards and Science (KRISS) has invested considerable effort in the controlled fabrication of CNT tips and is collaborating with the National Institute of Standards and Technology on the application of CNT tips for CD-AFM. Progress by KRISS on the precise control of CNT orientation, length, and end modification, using manipulation and focused ion beam processes, has allowed us to implement ball-capped CNT tips and bent CNT tips for CD-AFM. Using two different generations of CD-AFM instruments, we have evaluated these tip types by imaging a line/space grating and a programmed line edge roughness specimen. We concluded that these CNTs are capable of scanning the profiles of these structures, including re-entrant sidewalls, but there remain important challenges to address. These challenges include tighter control of tip geometry and careful optimization of scan parameters and algorithms for using CNT tips.

5.
Ultramicroscopy ; 162: 25-34, 2016 Mar.
Artigo em Inglês | MEDLINE | ID: mdl-26720439

RESUMO

In atomic force microscopy (AFM) metrology, the tip is a key source of uncertainty. Images taken with an AFM show a change in feature width and shape that depends on tip geometry. This geometric dilation is more pronounced when measuring features with high aspect ratios, and makes it difficult to obtain absolute dimensions. In order to accurately measure nanoscale features using an AFM, the tip dimensions should be known with a high degree of precision. We evaluate a new AFM tip characterizer, and apply it to critical dimension AFM (CD-AFM) tips used for high aspect ratio features. The characterizer is made up of comb-shaped lines and spaces, and includes a series of gratings that could be used as an integrated nanoscale length reference. We also demonstrate a simulation method that could be used to specify what range of tip sizes and shapes the characterizer can measure. Our experiments show that for non re-entrant features, the results obtained with this characterizer are consistent to 1nm with the results obtained by using widely accepted but slower methods that are common practice in CD-AFM metrology. A validation of the integrated length standard using displacement interferometry indicates a uniformity of better than 0.75%, suggesting that the sample could be used as highly accurate and SI traceable lateral scale for the whole evaluation process.