Detection and Analysis of Enamel Cracks by Quantitative Light-induced Fluorescence Technology.
Jun, Mi-Kyoung; Ku, Hye-Min; Kim, Euiseong; Kim, Hee-Eun; Kwon, Ho-Keun; Kim, Baek-Il.
  • Jun MK; Department of Preventive Dentistry and Public Oral Health, College of Dentistry, Yonsei University, Seoul, South Korea.
  • Ku HM; Department of Preventive Dentistry and Public Oral Health, College of Dentistry, Yonsei University, Seoul, South Korea; BK 21 PLUS Project, Yonsei University, College of Dentistry, Seoul, South Korea.
  • Kim E; Microscope Center, Department of Conservative Dentistry and Oral Science Research Center, College of Dentistry, Yonsei University, Seoul, South Korea.
  • Kim HE; Department of Dental Hygiene, Gachon University College of Health Science, Incheon, South Korea.
  • Kwon HK; Department of Preventive Dentistry and Public Oral Health, College of Dentistry, Yonsei University, Seoul, South Korea.
  • Kim BI; Department of Preventive Dentistry and Public Oral Health, College of Dentistry, Yonsei University, Seoul, South Korea; BK 21 PLUS Project, Yonsei University, College of Dentistry, Seoul, South Korea; Oral Science Research Institute, Yonsei University, College of Dentistry, Seoul, South Korea. Elect
J Endod ; 42(3): 500-4, 2016 Mar.
Article en En | MEDLINE | ID: mdl-26794344
INTRODUCTION: The ability to accurately detect tooth cracks and quantify their depth would allow the prediction of crack progression and treatment success. The aim of this in vitro study was to determine the capabilities of quantitative light-induced fluorescence (QLF) technology in the detection of enamel cracks. METHODS: Ninety-six extracted human teeth were selected for examining naturally existing or suspected cracked teeth surfaces using a photocuring unit. QLF performed with a digital camera (QLF-D) images were used to assess the ability to detect enamel cracks based on the maximum fluorescence loss value (ΔFmax, %), which was then analyzed using the QLF-D software. A histologic evaluation was then performed in which the samples were sectioned and observed with the aid of a polarized light microscope. The relationship between ΔFmax and the histology findings was assessed based on the Spearman rank correlation. The sensitivity and specificity were calculated to evaluate the validity of using QLF-D to analyze enamel inner-half cracks and cracks extending to the dentin-enamel junction. RESULTS: There was a strong correlation between the results of histologic evaluations of enamel cracks and the ΔFmax value, with a correlation coefficient of 0.84. The diagnostic accuracy of QLF-D had a sensitivity of 0.87 and a specificity of 0.98 for enamel inner-half cracks and a sensitivity of 0.90 and a specificity of 1.0 for cracks extending to the dentin-enamel junction. CONCLUSIONS: These results indicate that QLF technology would be a useful clinical tool for diagnosing enamel cracks, especially given that this is a nondestructive method.
Asunto(s)
Palabras clave

Texto completo: 1 Banco de datos: MEDLINE Asunto principal: Diente / Síndrome de Diente Fisurado / Esmalte Dental Tipo de estudio: Diagnostic_studies / Prognostic_studies Límite: Humans Idioma: En Año: 2016 Tipo del documento: Article

Texto completo: 1 Banco de datos: MEDLINE Asunto principal: Diente / Síndrome de Diente Fisurado / Esmalte Dental Tipo de estudio: Diagnostic_studies / Prognostic_studies Límite: Humans Idioma: En Año: 2016 Tipo del documento: Article