Your browser doesn't support javascript.
loading
Catalytic pyrolysis of harmful plastic waste to alleviate environmental impacts.
Yim, Hyunji; Valizadeh, Soheil; Rhee, Gwang Hoon; Jae, Jungho; Ali Khan, Moonis; Jeon, Byong-Hun; Nam, Hyungseok; Park, Young-Kwon.
  • Yim H; School of Environmental Engineering, University of Seoul, Seoul 02504, Republic of Korea.
  • Valizadeh S; School of Environmental Engineering, University of Seoul, Seoul 02504, Republic of Korea.
  • Rhee GH; Department of Mechanical and Information Engineering, University of Seoul, Seoul 02504, Republic of Korea.
  • Jae J; School of Chemial Engineering, Pusan National University, Busan 46241, Republic of Korea.
  • Ali Khan M; Chemistry Department, College of Science, King Saud University, Riyadh 11451, Saudi Arabia.
  • Jeon BH; Department of Earth Resource Environmental Engineering, Hanyang University, Seoul 04763, Republic of Korea.
  • Nam H; School of Mechanical Engineering, Kyungpook National University, Daegu 41566, Republic of Korea.
  • Park YK; School of Environmental Engineering, University of Seoul, Seoul 02504, Republic of Korea. Electronic address: catalica@uos.ac.kr.
Environ Pollut ; 343: 123198, 2024 Feb 15.
Article en En | MEDLINE | ID: mdl-38128713
ABSTRACT
Wax is a detrimental byproduct of plastic waste pyrolysis causing challenges upon its release into the environment owing to persistence and potential toxicity. In this study, the valorization of wax materials through conversion into BTEX (i.e., benzene, toluene, ethylbenzene, and xylene) was achieved via catalytic pyrolysis using zeolite-based catalysts. The potential of two types of waxes, spent wax (SW), derived from the pyrolysis of plastic waste, and commercial paraffin wax (PW), for BTEX generation, was investigated. Using HZSM-5, higher yields of oil (54.9 wt%) and BTEX (18.2 wt%) were produced from the pyrolysis of SW compared to PW (32.3 and 14.1 wt%, respectively). This is due to the improved accessibility of lighter hydrocarbons in SW to Brønsted and Lewis acid sites in HZSM-5 micropores, promoting cracking, isomerization, cyclization, Diels-Alder, and dehydrogenation reactions. Further, the use of HZSM-5 resulted in significantly larger yields of oil and BTEX from SW pyrolysis compared to Hbeta and HY. This phenomenon is ascribed to the well-balanced distribution of Brønsted and Lewis acid sites and the identical geometric structure of HZSM-5 micropores and BTEX molecules. The addition of Ga to HZSM-5 further led to 2.24% and 28.30% enhancements in oil and BTEX yields, respectively, by adjusting the acidity of the catalyst through the introduction of new Lewis acid sites. The regeneration of the Ga/HZSM-5 catalyst by removing deposited coke on the spent catalyst under air partially recovered catalytic activity. This study not only offers an efficient transformation of undesirable wax into valuable fuels but also provides an environmentally promising solution, mitigating pollution, contributing to carbon capture, and promoting a healthier and more sustainable environment. It also suggests future research directions, including catalyst optimization and deactivation management, feedstock variability exploration, and techno-economic analyses for sustainable wax conversion into BTEX via catalytic pyrolysis.
Asunto(s)
Palabras clave

Texto completo: 1 Banco de datos: MEDLINE Asunto principal: Pirólisis / Ácidos de Lewis Idioma: En Año: 2024 Tipo del documento: Article

Texto completo: 1 Banco de datos: MEDLINE Asunto principal: Pirólisis / Ácidos de Lewis Idioma: En Año: 2024 Tipo del documento: Article