ABSTRACT
Aim:
The aim of this in vitro study was to evaluate the surface roughness of three glass ionomer cements (GICs) indicated for ART restorations.Methods:
Ten cylindrical specimens of three commercial glass ionomers cements (Vidrion R - S.S. White, Maxxion R - FGM and Vitromolar DFL) were prepared (n=30) without surface finishing or protection. Twenty-four hours after preparation, the surface roughness measurements were obtained as the mean of three readings of the surface of each specimen by profilometry. The roughness values (Ra, ìm) were subjected to one-way ANOVA and Tukeys test (p<0.05).Results:
No statistically significant difference swere observed between Vidrion R (0.18 ± 0.05) and Vitromolar (0.21 ± 0.05), whereas Maxxion R presented significantly higher roughness values than those of the other materials.Conclusions:
It may be concluded that characteristics of particle size and composition of the different GICs affected their surface roughness 24 h after preparation.Palavras-chave
Texto completo:
1
Base de dados:
BBO
/
LILACS
Assunto principal:
Restauração Dentária Permanente
/
Tratamento Dentário Restaurador sem Trauma
/
Cimentos de Ionômeros de Vidro
Idioma:
En
Ano de publicação:
2010
Tipo de documento:
Article