Your browser doesn't support javascript.
loading
Lithiation of Crystalline Silicon As Analyzed by Operando Neutron Reflectivity.
Seidlhofer, Beatrix-Kamelia; Jerliu, Bujar; Trapp, Marcus; Hüger, Erwin; Risse, Sebastian; Cubitt, Robert; Schmidt, Harald; Steitz, Roland; Ballauff, Matthias.
Afiliação
  • Seidlhofer BK; Soft Matter and Functional Materials, Helmholtz-Zentrum Berlin für Materialien und Energie , Hahn-Meitner-Platz 1, 14109 Berlin, Germany.
  • Jerliu B; Institut für Metallurgie, Technische Universität Clausthal , AG Mikrokinetik, Robert-Koch-Str. 42, 38678 Clausthal-Zellerfeld, Germany.
  • Trapp M; Soft Matter and Functional Materials, Helmholtz-Zentrum Berlin für Materialien und Energie , Hahn-Meitner-Platz 1, 14109 Berlin, Germany.
  • Hüger E; Institut für Metallurgie, Technische Universität Clausthal , AG Mikrokinetik, Robert-Koch-Str. 42, 38678 Clausthal-Zellerfeld, Germany.
  • Risse S; Soft Matter and Functional Materials, Helmholtz-Zentrum Berlin für Materialien und Energie , Hahn-Meitner-Platz 1, 14109 Berlin, Germany.
  • Cubitt R; Institute Laue-Langevin , 71 avenue des Martyrs - CS 20156, 38042 Cedex 9 Grenoble, France.
  • Schmidt H; Institut für Metallurgie, Technische Universität Clausthal , AG Mikrokinetik, Robert-Koch-Str. 42, 38678 Clausthal-Zellerfeld, Germany.
  • Steitz R; Clausthaler Zentrum für Materialtechnik , Leibnizstraße 9, 38678 Clausthal-Zellerfeld, Germany.
  • Ballauff M; Soft Matter and Functional Materials, Helmholtz-Zentrum Berlin für Materialien und Energie , Hahn-Meitner-Platz 1, 14109 Berlin, Germany.
ACS Nano ; 10(8): 7458-66, 2016 08 23.
Article em En | MEDLINE | ID: mdl-27447734
ABSTRACT
We present an operando neutron reflectometry study on the electrochemical incorporation of lithium into crystalline silicon for battery applications. Neutron reflectivity is measured from the ⟨100⟩ surface of a silicon single crystal which is used as a negative electrode in an electrochemical cell. The strong scattering contrast between Si and Li due to the negative scattering length of Li leads to a precise depth profile of Li within the Si anode as a function of time. The operando cell can be used to study the uptake and the release of Li over several cycles. Lithiation starts with the formation of a lithium enrichment zone during the first charge step. The uptake of Li can be divided into a highly lithiated zone at the surface (skin region) (x ∼ 2.5 in LixSi) and a much less lithiated zone deep into the crystal (growth region) (x ∼ 0.1 in LixSi). The total depth of penetration was less than 100 nm in all experiments. The thickness of the highly lithiated zone is the same for the first and second cycle, whereas the thickness of the less lithiated zone is larger for the second lithiation. A surface layer of lithium (x ∼ 1.1) remains in the silicon electrode after delithiation. Moreover, a solid electrolyte interface is formed and dissolved during the entire cycling. The operando analysis presented here demonstrates that neutron reflectivity allows the tracking of the kinetics of lithiation and delithiation of silicon with high spatial and temporal resolution.
Palavras-chave

Texto completo: 1 Base de dados: MEDLINE Idioma: En Ano de publicação: 2016 Tipo de documento: Article

Texto completo: 1 Base de dados: MEDLINE Idioma: En Ano de publicação: 2016 Tipo de documento: Article