Radiopacity Evaluation of Gutta-Percha Points in Thinner Samples than the ANSI/ADA Recommendation.
Petry, Bruna Lucian; Bodanezi, Augusto; Baldasso, Flávia Emi Razera; Delai, Débora; Larentis, Naiara Leites; Fontanella, Vania Regina Camargo; Kopper, Patrícia Maria Poli.
Afiliação
  • Petry BL; Department of Conservative Dentistry, Dental School, UFRGS - Universidade Federal do Rio Grande do Sul, Porto Alegre, RS, Brazil.
  • Bodanezi A; Department of Conservative Dentistry, UFSC - Universidade Federal de Santa Catarina, Florianópolis, SC, Brazil.
  • Baldasso FER; Department of Conservative Dentistry, Dental School, UFRGS - Universidade Federal do Rio Grande do Sul, Porto Alegre, RS, Brazil.
  • Delai D; Department of Conservative Dentistry, Dental School, UFRGS - Universidade Federal do Rio Grande do Sul, Porto Alegre, RS, Brazil.
  • Larentis NL; Department of Radiology, ULBRA - Universidade Luterana do Brasil, Torres, RS, Brazil.
  • Fontanella VRC; Surgery and Orthopaedics Department, Dental School, UFRGS - Universidade Federal do Rio Grande do Sul, Porto Alegre, RS, Brazil.
  • Kopper PMP; Department of Conservative Dentistry, Dental School, UFRGS - Universidade Federal do Rio Grande do Sul, Porto Alegre, RS, Brazil.
Braz Dent J ; 28(5): 592-596, 2017.
Article em En | MEDLINE | ID: mdl-29215684
The aim of this study was to evaluate the radiopacity of different gutta-percha points (Endo Points®, Dentsply®, Tanari®, Meta®, Roeko® and Odous®) in samples of 1 mm thick as established by ANSI/ADA Specification #57 and ISO 6876/2001, in comparison with thinner samples. Twelve test specimens for each material, four for each thickness (0.3, 0.6, and 1 mm and diameter of 8 mm), were laminated and compressed between two polished glass plates until the desirable thickness. Digital radiographs were obtained along with a graduated aluminum stepwedge varying from 1 to 10 mm in thickness. The X-ray unit was set at 70 kVp, 10 mA and 0.4 s exposure time, at a focal distance of 36 cm. One calibrated observer quantified the average values of pixels with Adobe Photoshop® software. Data were analyzed using ANOVA and Tukey tests, at 5% significance level. At 0.6 and 1 mm thickness, all the tested materials showed radiopacity higher than 3 mm of aluminum (reference value). At 0.3 mm thickness, Odous and Tanari presented significantly less radiopacity than the reference, and the other materials showed similar radiopacity to the reference. The study concluded that the materials demonstrated different radiopacities and all had values above the minimum recommended by ANSI/ADA specification #57, being Odous and Tanari less radiopaque than the reference value in thinner samples (0.3mm).